Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 7.95 g/cc | 0.287 lb/in³ | |
Industeel CLC 17.12.2 L 2% Mo Containing 18 Cr –10 Ni Austenitic Stainless Steel Description: CLC 17-12-2L is one of the basic grade of the stainless steels range. 2% Molybdenum bearing ensures better corrosion resistance than CLC 18-9 L grade, particularly regarding to uniform .. |
|||
Density | 7.95 g/cc | 0.287 lb/in³ | |
Industeel CLC 17.13.3 LN Nitrogen Containing 18Cr-10Ni-2Mo Austenitic Stainless Steel Description: CLC 17-13-3LN is a nitrogen alloyed austenitic stainless steel with Mo additions. Its low carbon content avoids intergranular corrosion, even on welded pieces without an ulterior water .. |
|||
Density | 7.95 g/cc | 0.287 lb/in³ | |
Industeel CLC 18.10 Nb Niobium Stabilized 18Cr-10Ni Austenitic Stainless Steel CLC 18-10Nb is a 18Cr-10Ni austenitic stainless steel stabilized with specific Nb addition. This kind of steel is one of the basic grades of the stainless steels range. Niobium bearing and its low c.. |
|||
Density | 7.95 g/cc | 0.287 lb/in³ | |
Industeel CLC 18.10Ti Titanium-Stabilized 18Cr-10Ni Austenitic Stainless Steel CLC 18-10Ti is a 18Cr-9Ni austenitic stainless steel stabilized with some Titanium additions. This is a basic grades in the stainless steel range. Titanium bearing (carbide forming element) avoids i.. |
|||
Density | 7.95 g/cc | 0.287 lb/in³ | |
Carpenter BioDur™ 316LS Stainless Medical Implant Alloy, 35% Cold Worked Data provided by Carpenter Technology Corporation.Medical Implant Alloy. Vacuum arc remelted (VAR), low carbon version of Type 316 stainless. The secondary premium melting step (VAR) imparts impro.. |
|||
Density | 7.95 g/cc | 0.287 lb/in³ | |
Carpenter BioDur™ 316LS Stainless Medical Implant Alloy, 48% Cold Worked Data provided by Carpenter Technology Corporation.Medical Implant Alloy. Vacuum arc remelted (VAR), low carbon version of Type 316 stainless. The secondary premium melting step (VAR) imparts impro.. |
|||
Density | 7.95 g/cc | 0.287 lb/in³ | |
Carpenter BioDur™ 316LS Stainless Medical Implant Alloy, 52% Cold Worked Data provided by Carpenter Technology Corporation.Medical Implant Alloy. Vacuum arc remelted (VAR), low carbon version of Type 316 stainless. The secondary premium melting step (VAR) imparts impro.. |
|||
Density | 7.95 g/cc | 0.287 lb/in³ | |
Carpenter BioDur™ 316LS Stainless Medical Implant Alloy, 60% Cold Worked Data provided by Carpenter Technology Corporation.Medical Implant Alloy. Vacuum arc remelted (VAR), low carbon version of Type 316 stainless. The secondary premium melting step (VAR) imparts impro.. |
|||
Density | 7.95 g/cc | 0.287 lb/in³ | |
Carpenter BioDur™ 316LS Stainless Medical Implant Alloy, 70% Cold Worked Data provided by Carpenter Technology Corporation.Medical Implant Alloy. Vacuum arc remelted (VAR), low carbon version of Type 316 stainless. The secondary premium melting step (VAR) imparts impro.. |
|||
Density | 7.95 g/cc | 0.287 lb/in³ | |
Carpenter BioDur™ 316LS Stainless Medical Implant Alloy, 90% Cold Worked Data provided by Carpenter Technology Corporation.Medical Implant Alloy. Vacuum arc remelted (VAR), low carbon version of Type 316 stainless. The secondary premium melting step (VAR) imparts impro.. |
|||
Density | 7.95 g/cc | 0.287 lb/in³ | |
Carpenter BioDur™ 316LS Stainless Medical Implant Alloy, Annealed Data provided by Carpenter Technology Corporation.Medical Implant Alloy. Vacuum arc remelted (VAR), low carbon version of Type 316 stainless. The secondary premium melting step (VAR) imparts impro.. |
|||
Density | 7.95 g/cc | 0.287 lb/in³ | |
ATI Allegheny Ludlum Stainless Steel JS700® Alloy (UNS N08700) Allegheny Ludlum's Corrosion resistant engineering alloy, JS700®, is a high-alloy, fully austenitic, superaustenitic stainless steel. This alloy is a proven problem-solver in many applications whe.. |