Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 0.262 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 7.24 g/cc
0.262 lb/in³
Indium Corp. Indalloy 172 Tin Solder Alloy
Information Provided by Indium Corporation
Density 7.26 g/cc
0.262 lb/in³
Indium Corp. Indalloy 173 Tin Solder Alloy
Information Provided by Indium Corporation
Density 7.26 g/cc
0.262 lb/in³
Indium Corp. Indalloy® 131 97Sn/3Sb Lead-Free Solder Alloy
Information provided by the manufacturer, Indium Corporation.
Density 7.25 g/cc
0.262 lb/in³
Indium Corp. Indalloy® 133 Sn-Sb Solder Alloy
Higher tensile strength solder than #121. Particular application is joining copper tubing in refrigeration and potable water systems. Has good wettability with good long time sheer strength at 100Â..
Density 7.24 g/cc
0.262 lb/in³
Indium Corp. Indalloy 259 Tin Solder Alloy
Information Provided by Indium Corporation
Density 7.25 g/cc
0.262 lb/in³
Indium Corp. Indalloy® 227 Sn-In-Ag Solder Alloy
Pb free solder can be used as a replacement for 63Sn 37Pb, 62Sn 36Pb 2Ag and 60Sn 40Pb in that it has similar physical and mechanical properties. Not for use over 100°C due to 118°C Sn/In eut..
Density 7.25 g/cc
0.262 lb/in³
Special Metals INCOLOY® Alloy MA 956
An iron-chromium-aluminum alloy that is oxide dispersion strengthened and produced by mechanical alloying. Production involves high-energy milling of metal powders to create an alloy with a strengt..
Density 7.25 g/cc
0.262 lb/in³
Williams Advanced Alloys WS187 Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Density 7.25 g/cc
0.262 lb/in³
Williams Advanced Alloys WS240 Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Density 7.24 g/cc
0.262 lb/in³
American Elements Neodymium Oxide Nanopowder
General DescriptionND-MITE powders and dispersions are inorganic neodymium-oxide nanoparticles. ND-MITE-A products are uncoated and hydrophilic. ND-MITE-O products are coated with an organic silane ..
Density 7.25 g/cc
0.262 lb/in³
Crucible Steel CPM® 15V® Tool Steel
CPM 15V is intended for applications requiring exceptional wear resistance. It has more vanadium carbides in its microstructure than CPM 10V and provides more wear resistance and longer tool life in..
Density 7.25 g/cc
0.262 lb/in³
California Fine Wire Stablohm 812 Chromium, Aluminum, and Iron Resistance Wire
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Density 7.25 g/cc
0.262 lb/in³
Resistalloy International Fecralloy™ 135 Electrical Resistance Steel
Ferritic stainless steel with aluminum. Available as wire, bar, and strip. Used mainly for electrical elements in both industrial and domestic applications. Industrial applications vary from small ..