CPM 15V is intended for applications requiring exceptional wear resistance. It has more vanadium carbides in its microstructure than CPM 10V and provides more wear resistance and longer tool life in those applications where 10V has proven to be successful. CPM 15V also offers an alternative to solid carbide where carbide fails by fracture or where intricate tool design makes carbide difficult or risky to fabricate. The CPM (Crucible Particle Metallurgy) process produces very homogeneous, high quality steel characterized by superior dimensional stability, grindability, and toughness compared to steels produced by conventional processes.Information provided by Crucible Specialty Metals.
Physical Properties Metric English Comments
Density 7.25 g/cc
0.262 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 255 - 277
255 - 277
Annealed
Hardness, Rockwell C 61 - 63
61 - 63
Modulus of Elasticity 235 GPa
34100 ksi
Charpy Impact 11.0 J
8.11 ft-lb
Austenitizing Temperature- 1175°C
12.0 J
8.85 ft-lb
Austenitizing Temperature- 1120°C
Thermal Properties Metric English Comments
CTE, linear 10.5 µm/m-°C

@Temperature 21.0 - 93.0 °C
5.83 µin/in-°F

@Temperature 69.8 - 199 °F
11.1 µm/m-°C

@Temperature 21.0 - 260 °C
6.17 µin/in-°F

@Temperature 69.8 - 500 °F
12.1 µm/m-°C

@Temperature 21.0 - 593 °C
6.72 µin/in-°F

@Temperature 69.8 - 1100 °F
Component Elements Properties Metric English Comments
Carbon, C 3.4 %
3.4 %
Chromium, Cr 5.25 %
5.25 %
Iron, Fe 75.55 %
75.55 %
As Remainder
Molybdenum, Mo 1.3 %
1.3 %
Vanadium, V 14.5 %
14.5 %