Indium Corp. Indalloy® 133 Sn-Sb Solder Alloy

Category Metal , Nonferrous Metal , Solder/Braze Alloy , Tin Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy® 133 Sn-Sb Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Higher tensile strength solder than #121. Particular application is joining copper tubing in refrigeration and potable water systems. Has good wettability with good long time sheer strength at 100°C.Information provided by the manufacturer, Indium Corporation.
Physical Properties Metric English Comments
Density 7.25 g/cc
0.262 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 13.3
13.3
Tensile Strength, Ultimate 40.7 MPa
5900 psi
Elongation at Break 38 %
38 %
Shear Strength 41.4 MPa
6000 psi
Shear Bond Holding Strength
Thermal Properties Metric English Comments
CTE, linear 31.0 µm/m-°C

@Temperature 20.0 °C
17.2 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 28.0 W/m-K

@Temperature 85.0 °C
194 BTU-in/hr-ft²-°F

@Temperature 185 °F
Melting Point 235 - 240 °C
455 - 464 °F
Solidus 235 °C
455 °F
Liquidus 240 °C
464 °F
Component Elements Properties Metric English Comments
Antimony, Sb 5.0 %
5.0 %
Tin, Sn 95 %
95 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000140 ohm-cm
0.0000140 ohm-cm