Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.66 g/cc | 0.0960 lb/in³ | |
PCP-Canada ALCA 5® 5083 Cast Aluminum Mold Plate ALCA5® cast precision plate product has an excellent dimensional stability. The low level of internal stress reduces the plate deformation during and after machining. This high stability leads to c.. |
|||
Density | 2.66 g/cc | 0.0960 lb/in³ | |
Vista Metals ATP-5™ Precision Cast Aluminum Plate Used where flatness and dimensional control are critical, such as: computer & electronics, pharmaceuticals, medical testing equipment, packaging machinery, printing machinery, thermoforming tools, m.. |
|||
Density | 2.66 g/cc | 0.0960 lb/in³ | |
Vista Metals Duramold-5™ Cast Aluminum Mold Plate Used for molds for the automotive industry, blow molds, structural foam molds, rubber molds, low pressure injection molds, Thermoforming molds, R.I.M. and R.T.M. molding.Features: Excellent Machinab.. |
|||
Density | 2.66 g/cc | 0.0960 lb/in³ | |
Alpase K100-S™ Aluminum Plate K100-S™ features and benefits include: Dimensional stability, fully weldable, anodizable, high elongation, consistent properties - regardless of size, close flatness and tolerances, superior corros.. |
|||
Density | 2.66 g/cc | 0.0960 lb/in³ | |
Alpase M-5™ Aluminum Mold Plate Excellent weldabilitySurface Condition - Machined top and bottom to reduce costly handling and machining stepsDimensional Stability - High dimensional stability during and after machiningPolishing -.. |
|||
Density | 2.66 g/cc | 0.0960 lb/in³ | |
ALIMEX 5083 O/H111Aluminum Alloy Rolled Rolled aluminium material according to DIN EN standard. Information provided by ALIMEX GmbHAnnealed and slightly strain-hardened |
|||
Density | 2.66 g/cc | 0.0960 lb/in³ | |
ALIMEX ACP 5080 Aluminum Cast Plate ACP 5080 is a 5xxx series precision aluminum cast plate. Thickness, flatness and surface finish offer very tight tolerances.Material stability and excellent processing characteristics make this alum.. |
|||
Density | 2.66 g/cc | 0.0960 lb/in³ | |
ALIMEX PLANAL 5083 O/H111 Aluminum Alloy Aluminium rolled plates which have been machined on both sides. Has a precise surface finish and high tensile strength. The temper values and the material conditions are not changed by surface-machi.. |
|||
Density | 2.66 g/cc | 0.0960 lb/in³ | |
ALIMEX ACP 5080R Aluminum Cast Material Sizes range availability along with good mechanical and physical properties of ACP 5080R provide the Mold Tool Industry tooling materials solutions for the most challenging applications.Information .. |
|||
Density | 2.66 g/cc | 0.0960 lb/in³ | |
PCP-Canada Max 5® 5083 Cast Aluminum Mold Block Max 5® is characterized by an excellent dimensional stability. It is a 5083 alloy which provides strength, good hard anodizing response, weldability, and machinability (with sintered carbide materi.. |