Material Notes:
K100-S™ features and benefits include: Dimensional stability, fully weldable, anodizable, high elongation, consistent properties - regardless of size, close flatness and tolerances, superior corrosion resistance, can be nickel plated, smoothest aluminum surface finish.Applications:Can be painted on both sides, including heat-cured finishes; used for mold cooling and heating plates without impregnation; low pressure molds for shoes, skis, etc.; plate for composite tooling requiring vacuum integrity and dimensional stability.Sizes: Thickness 0.25 -8 inches; Width 38.25, 48.5, and 60.5 inches (custom up to 88 inches); Length 96.5 and - 144.5 inches. Data provided by Alpase.
Physical Properties Metric English Comments
Density 2.66 g/cc
0.0960 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 70
70
Tensile Strength, Ultimate 283 MPa
41000 psi
Typical
Tensile Strength, Yield 124 MPa
18000 psi
Typical
Elongation at Break 12 - 15 %
12 - 15 %
Typical
Modulus of Elasticity 71.0 GPa
10300 ksi
Thermal Properties Metric English Comments
CTE, linear 23.8 µm/m-°C

@Temperature 20.0 - 100 °C
13.2 µin/in-°F

@Temperature 68.0 - 212 °F
Thermal Conductivity 117 W/m-K
812 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Aluminum, Al 94 %
94 %
as balance
Copper, Cu 0.10 - 0.20 %
0.10 - 0.20 %
Iron, Fe 0.10 - 0.40 %
0.10 - 0.40 %
Magnesium, Mg 4.0 - 4.9 %
4.0 - 4.9 %
Manganese, Mn 0.40 - 1.0 %
0.40 - 1.0 %
Silicon, Si 0.00 - 0.40 %
0.00 - 0.40 %
Zinc, Zn 0.00 - 0.25 %
0.00 - 0.25 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000590 ohm-cm
0.00000590 ohm-cm