Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.0430 - 0.0630 g/cc | 0.00155 - 0.00228 lb/in³ | sheet density |
Zotefoams Plastazote® HD60 High Density Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Density | 0.0430 - 0.0580 g/cc | 0.00155 - 0.00210 lb/in³ | sheet density |
Zotefoams Plastazote® LD50CN Conductive Low Density Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Density | 0.0430 - 0.0550 g/cc | 0.00155 - 0.00199 lb/in³ | sheet density |
Zotefoams Plastazote® LD52 Low Density Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Density | 0.0430 - 0.0550 g/cc | 0.00155 - 0.00199 lb/in³ | typical range; ISO 845 |
3A Composites Core Materials AIREX® C70.48 Universal Structural Foam AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negligible .. |