Polymer Property : Density = 0.00155 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.0430 - 0.0630 g/cc
0.00155 - 0.00228 lb/in³
sheet density
Zotefoams Plastazote® HD60 High Density Polyethylene Foam
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Density 0.0430 - 0.0580 g/cc
0.00155 - 0.00210 lb/in³
sheet density
Zotefoams Plastazote® LD50CN Conductive Low Density Polyethylene Foam
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Density 0.0430 - 0.0550 g/cc
0.00155 - 0.00199 lb/in³
sheet density
Zotefoams Plastazote® LD52 Low Density Polyethylene Foam
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Density 0.0430 - 0.0550 g/cc
0.00155 - 0.00199 lb/in³
typical range; ISO 845
3A Composites Core Materials AIREX® C70.48 Universal Structural Foam
AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negligible ..