Description: Ultramid® 1C forms flexible, scratch-resistant coatings or tough, resilient, abrasion-resistant coverings on plastics, films, nonwovens, fabrics, leather, paper, wood, or metal.Information provided by BASF
Physical Properties Metric English Comments
Bulk Density 0.500 - 0.800 g/cc
0.0181 - 0.0289 lb/in³
Density 1.10 g/cc
0.0397 lb/in³
Mechanical Properties Metric English Comments
Ball Indentation Hardness 115 MPa
16700 psi
ISO 2039/1
Tensile Strength, Yield 80.0 MPa
11600 psi
ISO 527
Elongation at Yield 5.0 %
5.0 %
ISO 527
Tensile Modulus 1.40 GPa
203 ksi
ISO 527
Flexural Strength 47.0 MPa
6820 psi
ISO 178
Flexural Modulus 1.40 GPa
203 ksi
ISO 178
Charpy Impact Unnotched NB
NB
ISO 179/1eU
Thermal Properties Metric English Comments
Melting Point 185 °C
365 °F
Decomposition Temperature >= 300 °C
>= 572 °F
Descriptive Properties Value Comments
Commercial Status Europe
Ignition Temperature >400°C
ASTM D1929