Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.971 g/cc | 0.0351 lb/in³ | ASTM D1475 |
Humiseal 1C49 Silicone Conformal Coating Humiseal 1C49 Silicone Conformal CoatingHigh temperature resistanceGood dielectrical propertiesGood moisture resistanceRepairableUL ApprovedMIL-I-46058C ApprovedPasses thermal shock test (MIL-I-4605.. |
|||
Density | 0.971 - 1.03 g/cc | 0.0351 - 0.0372 lb/in³ | |
Lord Adhesives 521 Medium Viscosity, Slow Cure Acrylic Adhesive Lord 500 SeriesLord 500 Series Acrylic Adhesives bond plastics and prepared metals; they offer excellent adhesion to both thermoplastics and thermoset plastics. They are available with varying handi.. |
|||
Density | 0.971 - 1.02 g/cc | 0.0351 - 0.0368 lb/in³ | |
Lord Adhesives 660 White, Non Sag, Fast Set for FRP Acrylic Adhesive Lord Adhesives 660 White, Non Sag, Fast Set for FRP Acrylic AdhesiveLord 660 Acrylic Adhesive bonds FRP (fiber-reinforced plastics) with minimal surface preparation. Lord 660 can cross-bond FRP to m.. |
|||
Density | 0.971 g/cc | 0.0351 lb/in³ | Mixed |
ITW Plexus Plexusâ„¢ MA422 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose adhesive, medium open time.Information provided by Illinois Tool Works. |
|||
Density | 0.971 g/cc | 0.0351 lb/in³ | Mixed |
ITW Plexus Plexusâ„¢ MA820 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Excellent for structural bonding of surface metals with no surface preparation.Information provide.. |
|||
Density | 0.971 g/cc | 0.0351 lb/in³ | Mixed |
ITW Plexus Plexusâ„¢ MA920 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose, low odor, short open time.Information provided by Illinois Tool Works. |
|||
Density | 0.972 g/cc | 0.0351 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Catalyst CT/5-LR UV Polyolefin Catalyst CT/5-LR UV is a polyolefin based masterbatch to be used with cable silane crosslinkable compounds in the amount suggested for each material. Developed for Polidan®, Polidiemme® and Co.. |
|||
Density | 0.972 g/cc | 0.0351 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Catalyst CT/7 UV Polyolefin Catalyst CT/7 UV is a polyolefin based masterbatch to be used with cable silane crosslinkable compounds in the amount suggested for each material. Developed for Polidan®, Polidiemme® and Cogeg.. |
|||
Density | 0.972 g/cc | 0.0351 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Catalyst CT/7-LR UV Polyolefin Catalyst CT/7-LR UV is a polyolefin based masterbatch to be used with cable silane crosslinkable compounds in the amount suggested for each material. Developed for Polidan®, Polidiemme® and Co.. |
|||
Density | 0.972 g/cc | 0.0351 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Catalyst CT/5 UV Polyolefin Catalyst CT/5 is a polyolefin based masterbatch to be used with cable silane crosslinkable compounds in the amount suggested for each material. Developed for Polidan®, Polidiemme® and CogegumÂ.. |
|||
Density | 0.971 - 0.975 g/cc | 0.0351 - 0.0352 lb/in³ | BRCP 4843 |
ExxonMobil Jayflex™ DINP Plasticizer Appearance: Clear and FreeAvailability: AmericasCAS Number: 33703-08-01Information provided by ExxonMobil |
|||
Density | 0.972 g/cc | 0.0351 lb/in³ | |
Abatron Primkote G A/B Waterborne Epoxy Primer/Sealer for Green Concrete Primkote G is a waterborne epoxy system for priming and sealing floors. It contains a gray resin compound (Part A) and a clear hardener (Part B). It conditions concrete and other substrates for epox.. |
|||
Density | 0.971 g/cc | 0.0351 lb/in³ | |
3M Scotch-Weld™ General Purpose 60 CA Adhesive A low VOC general purpose industrial grade spray adhesiveFeatures:This adhesive brings value as it has exceptionally high solidsThis adhesive is designed for temporary or permanent bonds on substrat.. |
|||
Density | 0.971 g/cc | 0.0351 lb/in³ | AboCure 50-12 |
Abatron AboCast 7802-1/AboCure 50-12 Epoxy AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 50-12 is a clear converter for high rigidity, chemical, and temperature resistance (HDT: 101.. |
|||
Density | 0.971 g/cc | 0.0351 lb/in³ | Mixed |
ITW Plexus Plexus™ MA922 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose, low odor, medium open time.Information provided by Illinois Tool Works. |