Primkote G is a waterborne epoxy system for priming and sealing floors. It contains a gray resin compound (Part A) and a clear hardener (Part B). It conditions concrete and other substrates for epoxy and polyurethane coatings. It is an excellent tie-coat between old glossy epoxy and other cured coating for subsequent coatings. It offers the best recoat adhesion within the first 1-4 days. After this point, it should be sanded or reprimed with Primkote G if it is glossy and difficult to wet. It can also be used alone, in one or several coats, to protect a color pattern, etc. Primkote G offers: (1) Application to freshly poured concrete, within hours after the concrete has been poured; (2) Application to fully cured concrete; (3) Cancels out the necessity to wait 28 days or cure and shot-blast new concrete before it can be finished; (4) Very low viscosity for penetration and wetting; (5) Low VOC (meets EPA method 24); (6) Outstanding water and weather resistance; (7) Fast hardening time (1 1/4 hrs); (8) Gray color for improved visual inspection. Suggested Uses: Priming/Sealing of freshly poured concrete surfaces; Penetrating and Conditioning concrete for urethanes and tie-coats on epoxy surfaces; Gray-Colored Primer for floors.
Physical Properties Metric English Comments
Specific Gravity 1.08 g/cc
1.08 g/cc
Density 0.972 g/cc
0.0351 lb/in³
Solids Content 41.2 %
41.2 %
Viscosity 10.5 - 18 cP
10.5 - 18 cP
Processing Properties Metric English Comments
Pot Life 720 min
720 min
Descriptive Properties Value Comments
Hardening Time (min) 75
25°C
Hardness, pencil HB
Parts by Weight (pbw) 100
Part A
54.4
Part B
Tack-free Time (min) 45