AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 50-12 is a clear converter for high rigidity, chemical, and temperature resistance (HDT: 101°C). It has low viscosity (22-30 cps) and a weight of 8.1 lbs/gallon. AboCast 8702-1/AboCure 50-12 has versatility and tenacious adhesion to metals, ceramics, glass, wood, and most rigid materials which permits permanent structural and dielectric bonds. Absence of volatiles and minimum shrinkage, typical of solventless epoxy systems, allow castings and masses of virtually any desired thickness. Suggested Uses: Multi-purpose casting, coating, and bonding for applications requiring high dielectric resistance, structural strength, and radiation resistance as well as resistance to weather, water, alkalis, diluted acids, fuels, and most common solvents; it was originally developed for FERMILAB.
Physical Properties Metric English Comments
Density 0.971 g/cc
0.0351 lb/in³
AboCure 50-12
1.09 g/cc
0.0394 lb/in³
AboCast 7802-1
Water Absorption 0.10 - 0.20 %
0.10 - 0.20 %
Viscosity 300 - 500 cP
300 - 500 cP
blended
Mechanical Properties Metric English Comments
Hardness, Shore D 85

@Temperature 100 °C,
Time 10800 sec
85

@Temperature 212 °F,
Time 3.00 hour
85

@Temperature 100 °C,
Time 10800 sec
85

@Temperature 212 °F,
Time 3.00 hour
1/8 in thickness
75

@Time 86400 sec
75

@Time 24.0 hour
1/8 in thickness
75

@Time 259000 sec
75

@Time 72.0 hour
1/8 in thickness
80

@Time 3600 sec
80

@Time 1.00 hour
80

@Time 86400 sec
80

@Time 24.0 hour
80

@Time 259000 sec
80

@Time 72.0 hour
Tensile Strength at Break 82.7 - 96.5 MPa
12000 - 14000 psi
Elongation at Break 5.0 - 7.0 %
5.0 - 7.0 %
Flexural Strength 103 - 124 MPa
15000 - 18000 psi
Compressive Strength 75.8 - 82.7 MPa
11000 - 12000 psi
Electrical Properties Metric English Comments
Dielectric Strength 15.7 - 18.7 kV/mm
400 - 475 kV/in
Processing Properties Metric English Comments
Pot Life 45 min
45 min
100 g
Descriptive Properties Value Comments
Parts by Weight (pbw) 100
AboCast 7802-1
13
AboCure 50-12
Users viewing this material also viewed the following: