Polymer Property : Density = 0.972 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.972 g/cc
0.0351 lb/in³
ASTM D792
Solvay Specialty Polymers Catalyst CT/5-LR UV Polyolefin
Catalyst CT/5-LR UV is a polyolefin based masterbatch to be used with cable silane crosslinkable compounds in the amount suggested for each material. Developed for Polidan®, Polidiemme® and Co..
Density 0.972 g/cc
0.0351 lb/in³
ASTM D792
Solvay Specialty Polymers Catalyst CT/7 UV Polyolefin
Catalyst CT/7 UV is a polyolefin based masterbatch to be used with cable silane crosslinkable compounds in the amount suggested for each material. Developed for Polidan®, Polidiemme® and Cogeg..
Density 0.972 g/cc
0.0351 lb/in³
ASTM D792
Solvay Specialty Polymers Catalyst CT/7-LR UV Polyolefin
Catalyst CT/7-LR UV is a polyolefin based masterbatch to be used with cable silane crosslinkable compounds in the amount suggested for each material. Developed for Polidan®, Polidiemme® and Co..
Density 0.972 g/cc
0.0351 lb/in³
ASTM D792
Solvay Specialty Polymers Catalyst CT/5 UV Polyolefin
Catalyst CT/5 is a polyolefin based masterbatch to be used with cable silane crosslinkable compounds in the amount suggested for each material. Developed for Polidan®, Polidiemme® and CogegumÂ..
Density 0.972 g/cc
0.0351 lb/in³
Abatron Primkote G A/B Waterborne Epoxy Primer/Sealer for Green Concrete
Primkote G is a waterborne epoxy system for priming and sealing floors. It contains a gray resin compound (Part A) and a clear hardener (Part B). It conditions concrete and other substrates for epox..