Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.875 - 2.24 g/cc | 0.0316 - 0.0809 lb/in³ | Average value: 1.11 g/cc Grade Count:307 |
Overview of materials for Cyanoacrylate Adhesive This property data is a summary of similar materials in the MatWeb database for the category "Cyanoacrylate Adhesive". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Density | 0.875 - 0.899 g/cc | 0.0316 - 0.0325 lb/in³ | |
Lord Adhesives 7707 n-Butyl Acetate Surface Conditioner Lord Adhesion Enhancers/Surface ModifiersTo meet the unique bonding demands that accompany the use of difficult-to-bond materials, the Lord Corporation offers a full line of adhesion enhancers/surfa.. |
|||
Density | 0.875 g/cc | 0.0316 lb/in³ | |
Silon Tabond 3042 Impact Modifier for PA Tabond 3042 is a chemically modified Ethylene Copolymer/LLDPE.Information provided by Silon |
|||
Density | 0.874 g/cc @Temperature 15.0 °C |
0.0316 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil 46 Mobil EAL Envirosyn H Series Mobil EAL Envirosyn H Series oils are super premium, high performance fully synthetic environmentally aware hydraulic and circulating oils designed to provide outstanding performance in systems oper.. |
|||
Density | 0.875 g/cc @Temperature 15.0 °C |
0.0316 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil 75W-80 Mobilfluid LT Mobilfluid LT is an extra high performance multipurpose tractor lubricant engineered to meet or exceed tractor transmission, drivetrain, and hydraulic fluid requirements. This product is designed to.. |
|||
Density | 0.876 g/cc @Temperature 15.0 °C |
0.0316 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil Mobil Delvac 50 Synthetic Transmission Fluid Mobil Delvac Synthetic Transmission Fluid 50 is a fully synthetic, manual transmission lubricant engineered to meet the most demanding extended drain and OEM warranty requirements. It is recommended.. |
|||
Density | 0.875 g/cc @Temperature 15.6 °C |
0.0316 lb/in³ @Temperature 60.1 °F |
|
ExxonMobil Mobilarma 522 Mobilarma 500 Series oils are premium performance products primarily intended as run-in or lay-up lubricants, which provide effective rust preventive films on the internal surfaces of machinery. The.. |
|||
Density | 0.874 g/cc | 0.0316 lb/in³ | |
ConocoPhillips Syncon® 220 Synthetic R&O Oil Syncon R&O Oil is a premium quality, synthetic, rust and oxidation (R&O)-inhibited circulating oil developed for use in circulating systems, rotary air compressors, lightly loaded enclosed gear driv.. |
|||
Density | 0.874 g/cc @Temperature 15.6 °C |
0.0316 lb/in³ @Temperature 60.0 °F |
ASTM D4052 |
ExxonMobil Solvesso™ Aromatic 100 Aromatic Fluid Appearance: Clear/Transparent LiquidAvailability: North AmericaInformation provided by ExxonMobil |
|||
Density | 0.874 g/cc | 0.0316 lb/in³ | ASTM D792 |
Dow AFFINITY™ GA 1950 Polyolefin Plastomer (POP) AFFINITY™ GA 1950 Polyolefin Plastomer (POP) is produced via INSITE™ Technology from Dow Plastics. This product can be used in applications such as polymer modification (i.e. flow enhancement and.. |
|||
Density | 0.875 g/cc | 0.0316 lb/in³ | ASTM D792 |
Dow AFFINITY™ KC 8852G Polyolefin Plastomer (POP) AFFINITY™ KC 8852G is an ethylene-octene copolymer produced via INSITE™ Technology. This product offers excellent performance as a cling resin in one-sided stretch cling film applications. This .. |
|||
Density | 0.875 g/cc @Temperature 15.0 °C |
0.0316 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil 75W-80 Mobilfluid LT Mobilfluid LT is an extra high performance multipurpose tractor lubricant engineered to meet or exceed tractor transmission, drivetrain, and hydraulic fluid requirements. This product is designed to.. |
|||
Density | 0.876 g/cc @Temperature 15.0 °C |
0.0316 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil Mobil Delvac 50 Synthetic Transmission Fluid Mobil Delvac Synthetic Transmission Fluid 50 is a fully synthetic, manual transmission lubricant engineered to meet the most demanding extended drain and OEM warranty requirements. It is recommended.. |
|||
Density | 0.876 g/cc @Temperature 15.0 °C |
0.0316 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil Nuto 46 H Series Exxon Nuto H Series oils are premium quality anti-wear hydraulic oils intended for industrial and mobile service applications where anti-wear lubricants are required. They are formulated with high q.. |
|||
Density | 0.876 g/cc | 0.0316 lb/in³ | |
ConocoPhillips El Mar® Grade 15W-40 Geo Oil Description: Conoco El Mar® Geo Oil is a high-quality, rust- and oxidation-inhibited, nondetergent, ashless gas engine oil. It is formulated with high viscosity index paraffinic base oils blended w.. |
|||
Density | 0.874 g/cc | 0.0316 lb/in³ | |
ConocoPhillips El Mar® Grade 15W-40 Mid Ash Supreme Oil Description: Conoco El Mar® Mid Ash Supreme Oil is a premium-quality, mid ash gas engine oil recommended for naturally aspirated and moderately to highly turbocharged four-cycle gas engines, such a.. |
|||
Density | 0.875 g/cc | 0.0316 lb/in³ | |
ConocoPhillips Hydroclear® 150 Circulating Oil Description: Conoco Hydroclear Circulating Oil is a high-quality, rust-inhibited circulating oil formulated from premium Conoco hydrocracked base stocks. Hydroclear Circulating Oil is specially form.. |
|||
Density | 0.876 g/cc | 0.0316 lb/in³ | |
ConocoPhillips Hydroclear® 150 Multipurpose R&O Oil, AGMA Lubricant No. 4 Description: Conoco Hydroclear Multipurpose R&O Oil is a rust- and oxidationinhibited industrial oil with ashless wear protection formulated from premium Conoco hydrocracked base stocks. Hydroclear .. |
|||
Density | 0.874 g/cc | 0.0316 lb/in³ | |
ConocoPhillips Hydroclear® 68 2 EP gear Oil Description: Conoco Hydroclear EP Gear Oil is a premium extreme-pressure industrial gear lubricant with superior deposit control. Hydroclear EP Gear Oil is specially formulated with proprietary addi.. |
|||
Density | 0.874 g/cc | 0.0316 lb/in³ | |
ConocoPhillips Hydroclear® MV100 AW Hydraulic Fluid Description: Conoco Hydroclear AW Hydraulic Fluid is specifically designed for use in high-pressure systems which require greater wear protection and deposit control than that provided by standard a.. |
|||
Density | 0.875 g/cc | 0.0316 lb/in³ | |
ConocoPhillips 100M Gear Oil AGMA Lubricant No. 3EP Description: Conoco Gear Oil is a heavy-duty extreme-pressure industrial gear lubricant formulated from high-quality hydrocracked base stocks to provide excellent oxidation inhibition, EP load-carry.. |
|||
Density | 0.876 g/cc | 0.0316 lb/in³ | |
ConocoPhillips 68 Gear Oil AGMA Lubricant No. 2 EP Description: Conoco Gear Oil is a heavy-duty extreme-pressure industrial gear lubricant formulated from high-quality hydrocracked base stocks to provide excellent oxidation inhibition, EP load-carry.. |
|||
Density | 0.876 g/cc | 0.0316 lb/in³ | |
ConocoPhillips Hydroclear® MV150 AW Hydraulic Fluid Description: Conoco Hydroclear AW Hydraulic Fluid is specifically designed for use in high-pressure systems which require greater wear protection and deposit control than that provided by standard a.. |
|||
Density | 0.875 g/cc @Temperature 20.0 °C |
0.0316 lb/in³ @Temperature 68.0 °F |
|
Akzo Nobel Trigonox® 301 Polymerization Initiator Initiator for the production of controlled rheology polypropylene (CR-PP).Chemical description: 3,6,9-Triethyl-3,6,9-trimethyl-1,4,7-triperoxonane, 41% solution in isoparaffinic hydrocarbonsCAS Numb.. |
|||
Density | 0.875 g/cc | 0.0316 lb/in³ | |
3M Hi-Strength 90 Spray Adhesive-Low VOC An industrial grade high strength aerosol spray adhesive.Features:Bonds to a variety of substrates including decorative laminate, headliners, and soft foams.Typically used in construction, woodworki.. |
|||
Density | 0.875 g/cc @Temperature 0.000 °C |
0.0316 lb/in³ @Temperature 32.0 °F |
|
BorsodChem ONGRONOX INP 75 D peroxide-type initiator Chemical name: Bis-(3,5,5-trimethyl-hexanoyl)-peroxide, or Di-isononanoyl-peroxide.Mol. wt: 314.50 g/mol.Active oxygen content: 5.09 %.Deflegmation material: isododecane.Major decomposition products.. |
|||
Density | 0.875 g/cc | 0.0316 lb/in³ | ASTM D1505 |
M. Holland Company MAGMA® LM311-DX LLDPE
(discontinued **) Features: Good Processability, Good Puncture Resistance, Good Tear Strength, Good ToughnessProcessing Method: ExtrusionInformation provided by M. Holland. |
|||
Density | 0.876 g/cc @Temperature 15.0 °C |
0.0316 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil Nuto 46 H Series Exxon Nuto H Series oils are premium quality anti-wear hydraulic oils intended for industrial and mobile service applications where anti-wear lubricants are required. They are formulated with high q.. |
|||
Density | 0.874 g/cc | 0.0316 lb/in³ | |
ConocoPhillips Conoco® El Mar® Ashless Heavy Duty Oil, SAE Viscosity Grade 15W-40 Conoco® El Mar Ashless Heavy Duty is a high-quality, ashless, dispersant-detergent gas engine oil designed for use in naturally aspirated and moderately turbocharged 2-stroke cycle natural gas engi.. |
|||
Density | 0.875 g/cc @Temperature 20.0 °C |
0.0316 lb/in³ @Temperature 68.0 °F |
|
LyondellBasell PTB Propylene glycol tertiary butyl ether Information provided by Lyondell. |