Silon Tabond 3042 Impact Modifier for PA

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE
Manufacturer Silon
Trade Name Tabond
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Silon Tabond 3042 Impact Modifier for PA.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Tabond 3042 is a chemically modified Ethylene Copolymer/LLDPE.Information provided by Silon
Physical Properties Metric English Comments
Density 0.875 g/cc
0.0316 lb/in³
Melt Flow 2.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Thermal Properties Metric English Comments
Melting Point 123.2 °C
253.8 °F
DSC
Descriptive Properties Value Comments
Color White