Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.875 - 0.899 g/cc | 0.0316 - 0.0325 lb/in³ | |
Lord Adhesives 7707 n-Butyl Acetate Surface Conditioner Lord Adhesion Enhancers/Surface ModifiersTo meet the unique bonding demands that accompany the use of difficult-to-bond materials, the Lord Corporation offers a full line of adhesion enhancers/surfa.. |
|||
Density | 0.863 - 0.899 g/cc | 0.0312 - 0.0325 lb/in³ | |
Lord Adhesives AP-134 Reactive Polymer Primer or Adhesive for Polar Substrates Lord Adhesion Enhancers/Surface ModifiersTo meet the unique bonding demands that accompany the use of difficult-to-bond materials, the Lord Corporation offers a full line of adhesion enhancers/surfa.. |
|||
Density | 0.863 - 0.899 g/cc | 0.0312 - 0.0325 lb/in³ | |
Lord Adhesives Chemlok® AP-134 One-Coat Primer Chemlok® AP-134 is a clear, low viscosity, solventborne reactive primer which can function as a primer or adhesive for a variety of polar substrates. Substrates include: steel, aluminum, brass, E.. |