Akzo Nobel Trigonox® 301 Polymerization Initiator

Category Other Engineering Material , Catalyst/Initiator , Polymer
Manufacturer Akzo Nobel
Trade Name Trigonox®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Akzo Nobel Trigonox® 301 Polymerization Initiator.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Initiator for the production of controlled rheology polypropylene (CR-PP).Chemical description: 3,6,9-Triethyl-3,6,9-trimethyl-1,4,7-triperoxonane, 41% solution in isoparaffinic hydrocarbonsCAS Number: 24748-23-0Acronym: Tx 301Information provided by Akzo Nobel Polymer Chemicals.
Physical Properties Metric English Comments
Density 0.875 g/cc

@Temperature 20.0 °C
0.0316 lb/in³

@Temperature 68.0 °F
Viscosity 5.0 cP

@Temperature 20.0 °C
5.0 cP

@Temperature 68.0 °F
Molecular Weight 264.3 g/mol
264.3 g/mol
One Hour Half Life Temperature 146 °C
295 °F
Storage Temperature 10.0 - 40.0 °C
50.0 - 104 °F