Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.844 g/cc @Temperature 15.0 °C |
0.0305 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil Mobil Velocite 6 The Mobil Velocite Oil Numbered Series oils are premium performance products primarily designed for the lubrication of high-speed spindles in machine tools. They are also used in some critical hydra.. |
|||
Density | 0.845 g/cc @Temperature 15.0 °C |
0.0305 lb/in³ @Temperature 59.0 °F |
|
ExxonMobil Mobilarma 247 Mobilarma 200 Series products are premium quality rust preventive materials designed to protect metal surfaces from rust and corrosion. They are formulated using light-bodied petroleum solvents with.. |
|||
Density | 0.845 g/cc | 0.0305 lb/in³ | |
ConocoPhillips Syncon® 46 Synthetic AW Hydraulic Fluid 46 Description: Conoco Syncon Synthetic AW Hydraulic Fluid is a synthetic polyalphaolefin (PAO) antiwear fluid for hydraulic systems that operate at extreme temperatures. It is available in four ISO vi.. |
|||
Density | 0.844 g/cc @Temperature 15.0 °C |
0.0305 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil Mobil Velocite 6 The Mobil Velocite Oil Numbered Series oils are premium performance products primarily designed for the lubrication of high-speed spindles in machine tools. They are also used in some critical hydra.. |
|||
Density | 0.845 g/cc @Temperature 15.0 °C |
0.0305 lb/in³ @Temperature 59.0 °F |
|
ExxonMobil Mobilarma 247 Mobilarma 200 Series products are premium quality rust preventive materials designed to protect metal surfaces from rust and corrosion. They are formulated using light-bodied petroleum solvents with.. |
|||
Density | 0.845 - 0.850 g/cc | 0.0305 - 0.0307 lb/in³ | |
BASF Lupragen® N 100 DMCHA Dimethylcyclohexylamine Formula: C8H17NCAS: 98-94-2Description: Dimethylcyclohexylamine is a colorless to yellow liquid, with an amine-like odor. It is also miscible with water in all proportions.Synonyms: DMCHA, N,N-Dime.. |
|||
Density | 0.843 - 0.847 g/cc | 0.0305 - 0.0306 lb/in³ | ASTM D4052 |