Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Mobilarma 247

Category Fluid , Lubricant
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Mobilarma 247.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Mobilarma 200 Series products are premium quality rust preventive materials designed to protect metal surfaces from rust and corrosion. They are formulated using light-bodied petroleum solvents with polar rust preventive, water displacement and fingerprint neutralising additives. These rust preventives are easy to apply and easy to remove making their application less man-power intensive. Mobilarma 245 is suited for the thin-film protection of finely finished parts between machining operations, including operations where water-soluble cutting and grinding fluids have been used. It is also suitable for use just before parts are packaged for storage or shipment, or to "dry" parts as a temporary protection until a heavier rust preventive can be applied. Mobilarma 247 is the heavier duty rust preventive designed to provide long term protection under more adverse conditions.Protection of equipment during storage or while temporarily out of service; Coating of equipment in preparation for shipment
Physical Properties Metric English Comments
Density 0.845 g/cc

@Temperature 15.0 °C
0.0305 lb/in³

@Temperature 59.0 °F
Kinematic Viscosity at 40°C (104°F) 3.0 cSt
3.0 cSt
ASTM D445
Thermal Properties Metric English Comments
Flash Point 71.0 °C
160 °F
ASTM D92