ConocoPhillips Syncon® 46 Synthetic AW Hydraulic Fluid 46

Category Fluid , Lubricant , Polyalphaolefin (PAO)
Manufacturer ConocoPhillips
Trade Name Syncon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ConocoPhillips Syncon® 46 Synthetic AW Hydraulic Fluid 46.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Conoco Syncon Synthetic AW Hydraulic Fluid is a synthetic polyalphaolefin (PAO) antiwear fluid for hydraulic systems that operate at extreme temperatures. It is available in four ISO viscosity grades: 22, 32, 46 and 68.Information provided by ConocoPhillips.
Physical Properties Metric English Comments
Density 0.845 g/cc
0.0305 lb/in³
Viscosity Measurement 137
137
Viscosity Index
Saybolt Viscosity at 100°F 214 SUS
214 SUS
Saybolt Viscosity at 210°F 51 SUS
51 SUS
Kinematic Viscosity at 40°C (104°F) 46 cSt
46 cSt
Kinematic Viscosity at 100°C (212°F) 7.6 cSt
7.6 cSt
ASTM Color 1.0
1.0
Thermal Properties Metric English Comments
Pour Point -56.7 °C
-70.0 °F
Flash Point 254 °C
490 °F
Electrical Properties Metric English Comments
Dielectric Strength 40.0 kV/mm
1020 kV/in
No thickness given
Chemical Properties Metric English Comments
Total Acid Number 0.70
0.70
Descriptive Properties Value Comments
ASTM Rust A&B Pass
Copper Corrosion 1A
Emulsion Characteristics (40-37-3) Max 5 minutes
Vickers 35VQ-25 Pump Test Pass