Material Notes:
CAS Number: 68526-86-3EINECS Number: 2712356Information provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.843 - 0.847 g/cc
0.0305 - 0.0306 lb/in³
ASTM D4052
Maximum Moisture Content 0.10
0.10
ISO 12937
Chemical Properties Metric English Comments
Acid Value <= 0.030
<= 0.030
[mg KOH/g]; ASTM D1045
Descriptive Properties Value Comments
Acidity <0.003%
as acetic acid, BRCP 4581
Carbonyl Number <0.2 mg KOH/g
ASTM E411
Color <10
Platinum Cobalt, ASTM D5386
Composition C14
<10%, ROP 104
C9+C10
<2.0%, ROP 104
Lights
<0.5%, ROP 104
Hydroxyl Number 275-295 mg KOH/g
ISO 1843-5
Purity >98.5%
BRCP 5287