Polymer Property : Density = 0.0300 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.830 - 0.870 g/cc
0.0300 - 0.0314 lb/in³
RP-17617
Solvay RHODOLINE® LC-2 Surfactant
Description: Highly efficient mineral oil based defoamers for flat to gloss paints, quick process foam know down and high in-can persistency.Identification: DEFOAMER BLENDAvailable in: North America..
Density 0.831 - 0.834 g/cc

@Temperature 20.0 °C
0.0300 - 0.0301 lb/in³

@Temperature 68.0 °F
Unipetrol Ethylhexanol
2-ethylhexanol is produced by propylene oxonation to n-butyraldehyde and by subsequent aldolization and hydrogenation. It is a transparent, colourless, flammable liquid of a characteristic odour, ha..
Density 0.832 g/cc

@Temperature 15.0 °C
0.0300 lb/in³

@Temperature 59.0 °F
ASTM D4052
ExxonMobil Exxsol™ D120 Dearomatized Fluid
Availability: Africa & Middle East and Europe Appearance: Clear/Transparent LiquidInformation provided by ExxonMobil
Density 0.830 g/cc
0.0300 lb/in³
DuPont™ Nomex® N196 Paper, 20 mil Nominal Thickness
Nomex® Type N196 is a high floc grade of Nomex® paper. This leads to a high degree of saturability combined with high stiffness and mechanical properties. Type N196 is used where good saturabili..
Density 0.830 g/cc
0.0300 lb/in³
ISO 1183
Ensinger TECANYL™ MT Autoclavable Polymer
TECANYL™ MT is a new family of autoclavable materials developed for medical device applications. The material offers the desired performance properties of PPSU based resins with the machining ease..
Density 0.830 g/cc
0.0300 lb/in³
ISO 1183
Ensinger TECANYL™ MT XRO Autoclavable Polymer
TECANYL™ MT is a new family of autoclavable materials developed for medical device applications. The material offers the desired performance properties of PPSU based resins with the machining ease..
Density 0.830 g/cc
0.0300 lb/in³
ASTM C134
BNZ Materials BNZP-26A Insulating Firebrick (French Grade)
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Density 0.830 - 0.870 g/cc
0.0300 - 0.0314 lb/in³
RP-17617
Solvay RHODOLINE® 643 Surfactant
Description :Highly efficient mineral oil based defoamers for flat to gloss paints, quick process foam know down and high in-can persistency.Identification: OIL BASE DEFOAMERAvailable in: North Amer..