Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.832 g/cc @Temperature 15.0 °C |
0.0300 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil Exxsol™ D120 Dearomatized Fluid Availability: Africa & Middle East and Europe Appearance: Clear/Transparent LiquidInformation provided by ExxonMobil |