Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.830 - 0.870 g/cc | 0.0300 - 0.0314 lb/in³ | RP-17617 |
Solvay RHODOLINE® LC-2 Surfactant Description: Highly efficient mineral oil based defoamers for flat to gloss paints, quick process foam know down and high in-can persistency.Identification: DEFOAMER BLENDAvailable in: North America.. |
|||
Density | 0.850 - 0.870 g/cc @Temperature 15.0 °C |
0.0307 - 0.0314 lb/in³ @Temperature 59.0 °F |
|
Unipetrol BTX fraction BTX fraction is manufactured by distillation of pyrolysis petrol. It is yellowish, highly combustible and easily inflammable liquid with strong aromatic odour. BTX fraction is mixture of aromatic hy.. |
|||
Density | 0.830 - 0.870 g/cc | 0.0300 - 0.0314 lb/in³ | RP-17617 |
Solvay RHODOLINE® 643 Surfactant Description :Highly efficient mineral oil based defoamers for flat to gloss paints, quick process foam know down and high in-can persistency.Identification: OIL BASE DEFOAMERAvailable in: North Amer.. |
|||
Density | 0.839 - 0.869 g/cc | 0.0303 - 0.0314 lb/in³ | |
Lord Adhesives Chemlok® Y-1540 Silicone Rubber Adhesive Chemlok® Y-1540 is a one-coat adhesive used to bond peroxide curing silicone, EPDM, and fluoroelastomers to cold rolled and phosphatized steel.All information provided by Lord. |