Material Notes:
TECANYL™ MT is a new family of autoclavable materials developed for medical device applications. The material offers the desired performance properties of PPSU based resins with the machining ease and tool friendliness of acetal or POM. This allows part designers to take advantage of lower manufacturing costs by increasing output rates, and reducing tool wear, all without sacrificing part performance. TECANYL™ MT and TECANYL™ MT XRO shapes are all ISO 10993 tested to support their use in instrumentation that is intended to come in contact with blood and tissure for a period of not more than 24 hours. Ensinger can also provide TECANYL™ MT grades in finished injection molded parts for high volume applications.Excellent autoclave performance comparable to higher temperature materialsEasily machined, producing high quality surfaceNo black speck generation as in sulfone polymersLower manufacturing costsISO 10993 TestedInformation Provided by Ensinger Industries, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.08 g/cc
1.08 g/cc
ASTM D792
Density 0.830 g/cc
0.0300 lb/in³
ISO 1183
Water Absorption 0.23 %

@Temperature 22.8 °C
0.23 %

@Temperature 73.0 °F
equilibrium; ISO 62
Mechanical Properties Metric English Comments
Tensile Strength at Break 67.6 MPa

@Temperature 22.8 °C
9800 psi

@Temperature 73.0 °F
ASTM D638
Elongation at Break 16.3 %

@Temperature 22.8 °C
16.3 %

@Temperature 73.0 °F
ASTM D638
Tensile Modulus 3.25 GPa

@Temperature 22.8 °C
471 ksi

@Temperature 73.0 °F
ASTM D638
Flexural Strength 101 MPa

@Temperature 22.8 °C
14600 psi

@Temperature 73.0 °F
ASTM D790
Flexural Modulus 2.54 GPa

@Temperature 22.8 °C
368 ksi

@Temperature 73.0 °F
ASTM D790
Izod Impact, Notched 1.39 J/cm

@Temperature 22.8 °C
2.60 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 86.6 µm/m-°C

@Temperature -40.0 - 37.8 °C
48.1 µin/in-°F

@Temperature -40.0 - 100 °F
ASTM E831
Deflection Temperature at 1.8 MPa (264 psi) 147 °C
296 °F
ASTM D648
Vicat Softening Point 75.6 °C
168 °F