Physical Properties Metric English Comments
Density >= 0.0300 g/cc
>= 0.00108 lb/in³
Minimum achievable; Single stage pre-expansion in continuous expander at atmospheric pressure
NOVA Chemicals Dytherm® 340R Expandable Polystyrene
This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved therma..
Density 0.0300 - 0.100 g/cc
0.00108 - 0.00361 lb/in³
Normal molded density assuming cost optimized selection of processing conditions.
NOVA Chemicals Dytherm® 340R Expandable Polystyrene
This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved therma..
Density >= 0.0300 g/cc
>= 0.00108 lb/in³
Minimum achievable; Single stage pre-expansion in continuous expander at atmospheric pressure
NOVA Chemicals Dytherm® 350R Expandable Polystyrene
This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved therma..
Density 0.0300 - 0.100 g/cc
0.00108 - 0.00361 lb/in³
Normal molded density assuming cost optimized selection of processing conditions.
NOVA Chemicals Dytherm® 350R Expandable Polystyrene
This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved therma..
Density 0.0300 g/cc
0.00108 lb/in³
0.6 minute residence time
Jackon JACKOCELL® S3312 Expanded Polystyrene Packaging and Shape Molding
100% Polystyrene.Pre-expansionA substantial reduced pentane emission has been made possible with Jackocell® S3312 - which will lead the industry into the future. High stability of pre-expanded be..
Density 0.0300 g/cc
0.00108 lb/in³
SPHERE ONE EXTENDOSPHERESâ„¢ PM 6550 Hollow Plastic Spheres
PM 6550 PM 6550 is an extremely light and versatile hollow sphere. Its plastic composition results in a very low density product. Only a very small amount of this hollow sphere is needed to provide ..
Density 0.0300 g/cc
0.00108 lb/in³
Nominal skin/skin; BS ISO 7214 1998
Zotefoams Evazote® EV30 Ethylene Vinyl Acetate Copolymer Foam
Evazote® is a closed cell, cross-linked EVA copolymer foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outsta..
Density 0.0300 g/cc
0.00108 lb/in³
Nominal skin/skin; BS ISO 7214 1998
Zotefoams Plastazote® HD30 High Density Polyethylene Foam
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Density 0.0300 g/cc
0.00108 lb/in³
Nominal skin/skin; BS ISO 7214 1998
Zotefoams Plastazote® LD30SD Static Dissipative Low Density Polyethylene Foam
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Density 0.0300 - 0.0390 g/cc
0.00108 - 0.00141 lb/in³
sheet density
Zotefoams Plastazote® HL34 Polyethylene Foam
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Density 0.0300 g/cc
0.00108 lb/in³
ISO 845
Zotefoams ZOTEK® F 30 PVDF Foam
Zotek® F 30 is a closed cell foam made from Arkema Kynar® PVDF manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and o..
Density <= 0.0300 g/cc
<= 0.00108 lb/in³
TMA
Akzo Nobel Expancel® 461 DU 20 Dry unexpanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
Density <= 0.0300 g/cc
<= 0.00108 lb/in³
TMA
Akzo Nobel Expancel® 461 WU 20 Wet unexpanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
Density 0.0300 g/cc
0.00108 lb/in³
ISO 845
BASF Neopolen® P 8220 K 0.03 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 8220 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 8220 K.Note: In order to..
Density 0.0300 g/cc
0.00108 lb/in³
ISO 845
BASF Neopolen® P 8225 K 0.03 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 8225 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 8225 K.Note: In order to..
Density 0.0300 g/cc
0.00108 lb/in³
BASF E-por® 0.03 g/cc Density; Styrene and Ethylene (Europe)
Description: Expandable granules made of styrene and ethylene containing polymers without flame retardant (blowing agent: pentane).Application: For the production of elastic, multi-shock absorbing e..
Density 0.0300 g/cc
0.00108 lb/in³
ISO 845
BASF Neopolen® P 9225 K 0.03 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9225 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9225 K.Note: In order to..
Density 0.0300 g/cc
0.00108 lb/in³
ISO 845
BASF Neopolen® P 8015 0.03 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 8015 is expanded Polypropylene supplied in the form of beads. The cells are largely closed. Physical properties of moldings made from Neopolen® P 8015Note: In order to mea..
Density 0.0300 g/cc
0.00108 lb/in³
BASF Styrodur® 2800 C Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Density 0.0300 g/cc
0.00108 lb/in³
BASF Styrodur® 3035 CN Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Density >= 0.0300 g/cc
>= 0.00108 lb/in³
Minimum achievable; Single stage pre-expansion in continuous expander at atmospheric pressure
Ineos Nova W441A Expandable Polystyrene
A regular molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, typically used for high density foam applications.Applications: This grade is sued mainly for..
Density 0.0300 - 0.0800 g/cc
0.00108 - 0.00289 lb/in³
Normal molded density assuming cost optimized selection of processing conditions.
Ineos Nova W441A Expandable Polystyrene
A regular molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, typically used for high density foam applications.Applications: This grade is sued mainly for..
Density >= 0.0300 g/cc
>= 0.00108 lb/in³
Minimum achievable; Single stage pre-expansion in continuous expander at atmospheric pressure
NOVA Chemicals Styrocell® D933A Expandable Polystyrene  (discontinued **)
This grade is a special molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, typically used for dry molding of drinking cups and thin wall containers.Applic..