Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.0290 - 0.0390 g/cc | 0.00105 - 0.00141 lb/in³ | sheet density |
Zotefoams Evazote® VA35 Ethylene Vinyl Acetate Copolymer Foam Evazote® is a closed cell, cross-linked EVA copolymer foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outsta.. |
|||
Density | 0.0300 - 0.0390 g/cc | 0.00108 - 0.00141 lb/in³ | sheet density |
Zotefoams Plastazote® HL34 Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Density | 0.0330 - 0.0390 g/cc | 0.00119 - 0.00141 lb/in³ | |
Akzo Nobel Expancel® 461 WE 20 d36 Wet expanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Density | 0.0330 - 0.0390 g/cc | 0.00119 - 0.00141 lb/in³ | |
Akzo Nobel Expancel® 551 WE 40 d36 Wet expanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Density | 0.0330 - 0.0390 g/cc | 0.00119 - 0.00141 lb/in³ | |
Akzo Nobel Expancel® 551 WE 80 d36 Wet expanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |