Physical Properties Metric English Comments
Density 0.0220 - 0.0350 g/cc
0.000795 - 0.00126 lb/in³
Usual Use
NOVA Chemicals Gedexcel® 25C Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent. Production of complex and high definition preform for the "lost foam" costing technique used in foundries.Information provided by NOV..
Density 0.0220 - 0.0500 g/cc
0.000795 - 0.00181 lb/in³
Usual Use
NOVA Chemicals Gedexcel® 35B Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent. Production of complex and high definition preforms for the "lost foam" casting technique used in foundries.Information provided by NO..
Density 0.0220 - 0.0800 g/cc
0.000795 - 0.00289 lb/in³
Polimeri Europa Extir® EH 2000 Expandable Polystyrene
Extir EH 2000 is an expandable polystyrene in the form of spherical beads of fine particle size, with a low pentane content as blowing agent. Extir does not contain CFC or HCFC. Extir EH 2000 is use..
Density 0.0220 - 0.0600 g/cc
0.000795 - 0.00217 lb/in³
Polimeri Europa Extir® P 1212 Expandable Polystyrene  (discontinued **)
Extir P 1212 is an expandable polystyrene in the form of spherical beads of very fine particle size and narrow distribution, containing pentane as blowing agent. Extir does not contain CFC or HCFC. ..
Density 0.0220 - 0.0600 g/cc
0.000795 - 0.00217 lb/in³
Density range normally used
Polimeri Europa Extir® P 1212 Expandable Polystyrene, Special Purpose  (discontinued **)
Particle size range is 0.2 - 0.5 mm. Minimum apparent density on a discontinuous pre-expander is 21 g/l. Minimum apparent density on a continuous pre-expander is 25 g/l.Processing technology used ..
Density 0.0220 - 0.0500 g/cc
0.000795 - 0.00181 lb/in³
Final Product Density
Iran Petrochemical (PCC) TPC - 522 FC Expandable Polystyrene
TPC - 522 FCApplications: shape molding with wall thickness
Density 0.0220 - 0.0500 g/cc
0.000795 - 0.00181 lb/in³
Final Product Density
Iran Petrochemical (PCC) TPC - 526 WP Expandable Polystyrene
TPC - 526 WPApplications: very thin-wall water proof shape molding products with wall thickness
Density 0.0220 g/cc
0.000795 lb/in³
2.5 minute residence time
Jackon JACKOCELL® S3312 Expanded Polystyrene Packaging and Shape Molding
100% Polystyrene.Pre-expansionA substantial reduced pentane emission has been made possible with Jackocell® S3312 - which will lead the industry into the future. High stability of pre-expanded be..
Density 0.0220 - 0.0280 g/cc
0.000795 - 0.00101 lb/in³
Akzo Nobel Expancel® 461 DE 40 d25 Dry expanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
Density 0.0220 - 0.0280 g/cc
0.000795 - 0.00101 lb/in³
Akzo Nobel Expancel® 461 DET 40 d25 Dry expanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
Density >= 0.0220 g/cc
>= 0.000795 lb/in³
Minimum achievable; Single stage pre-expansion in continuous expander at atmospheric pressure
NOVA Chemicals Styrocell® D733A Expandable Polystyrene  (discontinued **)
This grade is a special molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, typically used for contour molding.Applications: This grade is used for dry mol..