Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Trade Name : TECHNYLSTAR™ Product List

Category Nylon 66, Unreinforced , Nylon 6, 50% Glass Fiber Filled , Nylon 6, 60% Glass Fiber Filled , Nylon 6, 30% Glass Fiber Filled , Nylon 6, 40% Glass Fiber Filled , Nylon 6, 40% Mineral Filled , Nylon 66, 40% Mineral Filled , Nylon 6, Glass/Mineral Reinforced
Manufacturer Solvay
Tips: 50 items are displayed at most. For the rest of the results, please contact customer service.
PRODUCT NO. Category
Solvay TECHNYLSTARâ„¢ A205 F Natural S PA6, Eh 0 Nylon 66, Unreinforced
Solvay TECHNYLSTARâ„¢ A205 F Natural S PA66, Eh 50 Nylon 66, Unreinforced
Solvay TECHNYLSTARâ„¢ AFX 218 V50 PA6, 50% glass filled, Conditioned Nylon 6, 50% Glass Fiber Filled
Solvay TECHNYLSTARâ„¢ AFX 218 V50 PA6, 50% glass filled, DRY Nylon 6, 50% Glass Fiber Filled
Solvay TECHNYLSTARâ„¢ AFX 218 V60 PA6, 60% glass filled, Conditioned Nylon 6, 60% Glass Fiber Filled
Solvay TECHNYLSTARâ„¢ AFX 218 V60 PA6, 60% glass filled, DRY Nylon 6, 60% Glass Fiber Filled
Solvay TECHNYLSTARâ„¢ AFX 218S V50 PA6, 50% glass filled, DRY Nylon 6, 50% Glass Fiber Filled
Solvay TECHNYLSTARâ„¢ S 216 V30 PA6, 30% glass filled, Conditioned Nylon 6, 30% Glass Fiber Filled
Solvay TECHNYLSTARâ„¢ S 216 V30 PA6, 30% glass filled, DRY Nylon 6, 30% Glass Fiber Filled
Solvay TECHNYLSTARâ„¢ S 216 V35 PA6, 35% glass filled, Conditioned Nylon 6, 40% Glass Fiber Filled
Solvay TECHNYLSTARâ„¢ S 216 V35 PA6, 35% glass filled, DRY Nylon 6, 40% Glass Fiber Filled
Solvay TECHNYLSTARâ„¢ S 216L2 V30 PA6, 30% glass filled, Conditioned Nylon 6, 30% Glass Fiber Filled
Solvay TECHNYLSTARâ„¢ S 216L2 V30 PA6, 30% glass filled, DRY Nylon 6, 30% Glass Fiber Filled
Solvay TECHNYLSTARâ„¢ S 218 MT PA6, 40% mineral filled, Conditioned Nylon 6, 40% Mineral Filled
Solvay TECHNYLSTARâ„¢ S 218 MT PA6, 40% mineral filled, DRY Nylon 66, 40% Mineral Filled
Solvay TECHNYLSTARâ„¢ S 218 MZ20 V10 Black 2N PA6, 20% mineral, 10% glass filled, DRY Nylon 6, Glass/Mineral Reinforced
Solvay TECHNYLSTARâ„¢ S 218 V30 PA6, 30% glass filled, Conditioned Nylon 6, 30% Glass Fiber Filled
Solvay TECHNYLSTARâ„¢ S 218 V30 PA6, 30% glass filled, DRY Nylon 6, 30% Glass Fiber Filled
Solvay TECHNYLSTARâ„¢ S 218 V35 PA6, 35% glass filled, Conditioned Nylon 6, 40% Glass Fiber Filled
Solvay TECHNYLSTARâ„¢ S 218 V35 PA6, 35% glass filled, DRY Nylon 6, 40% Glass Fiber Filled
Solvay TECHNYLSTARâ„¢ S 60G1 V30 PA6, 30% glass filled, Conditioned Nylon 6, 30% Glass Fiber Filled
Solvay TECHNYLSTARâ„¢ S 60G1 V30 PA6, 30% glass filled, DRY Nylon 6, 30% Glass Fiber Filled
Solvay TECHNYLSTARâ„¢ SX 216 L2 V60 PA6, 60% glass filled, DRY Nylon 6, 60% Glass Fiber Filled
Solvay TECHNYLSTARâ„¢ SX 216 V50 PA6, 50% glass filled, Conditioned Nylon 6, 50% Glass Fiber Filled
Solvay TECHNYLSTARâ„¢ SX 216 V50 PA6, 50% glass filled, DRY Nylon 6, 50% Glass Fiber Filled
Solvay TECHNYLSTARâ„¢ SX 216 V60 PA6, 60% glass filled, Conditioned Nylon 6, 60% Glass Fiber Filled
Solvay TECHNYLSTARâ„¢ SX 216 V60 PA6, 60% glass filled, DRY Nylon 6, 60% Glass Fiber Filled
Solvay TECHNYLSTARâ„¢ SX 218 L2 V60 Black JA6A PA6, 60% glass filled, Conditioned Nylon 6, 60% Glass Fiber Filled
Solvay TECHNYLSTARâ„¢ SX 218 V50 BK 38N-K PA6, 50% glass filled, DRY Nylon 6, 50% Glass Fiber Filled
Solvay TECHNYLSTARâ„¢ SX 218 V50 PA6, 50% glass filled, Conditioned Nylon 6, 50% Glass Fiber Filled
Solvay TECHNYLSTARâ„¢ SX 218 V50 PA6, 50% glass filled, DRY Nylon 6, 50% Glass Fiber Filled
Solvay TECHNYLSTARâ„¢ SX 218 V60 Black Z PA6, 60% glass filled, Conditioned Nylon 6, 60% Glass Fiber Filled
Solvay TECHNYLSTARâ„¢ SX 218 L2 V60 Black JA6A PA6, 60% glass filled, DRY Nylon 6, 60% Glass Fiber Filled
Solvay TECHNYLSTARâ„¢ SX 218 V60 Black Z PA6, 60% glass filled, DRY Nylon 6, 60% Glass Fiber Filled
Copyright © lookpolymers.com All Rights Reserved