| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 20.3 g/cc | 0.733 lb/in³ |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Vickers | 110 | 110 | HV5; glowed |
| Tensile Strength, Ultimate | 320 MPa | 46400 psi | |
| Elongation at Break | 25 % | 25 % |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 1730 - 1750 °C | 3150 - 3180 °F | |
| Solidus | 1730 °C | 3150 °F | |
| Liquidus | 1750 °C | 3180 °F |
| Component Elements Properties | Metric | English | Comments |
|---|---|---|---|
| Copper, Cu | 4.0 % | 4.0 % | |
| Platinum, Pt | 96 % | 96 % |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Processing Temperature | 1000 °C | 1832 °F | Cuvette Temp |
| Casting Temperature | 1850 - 1950 °C | 3360 - 3540 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Color | platinum-white |