ATOFINA 8650 is a low melting, high ethylene random copolymer with improved color, optics and impact properties. The low melting point of ATOFINA 8650 makes it an excellent heat seal layer for oriented films. ATOFINA 8650 complies with FDA regulations Title 21 CFR Section 177. 1520(c) 3.1 and may be used under these provisions for food contact and packaging.ApplicationATOFINA 8650 is recommended for use in non-oriented film processes for manufacture of package films that require improved optical and impact properties and as a heat seal layer for oriented films. Information provided provided by Total Petrochemicals.Total Petrochemicals acquired former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Density 0.890 g/cc
0.0322 lb/in³
ASTM D1505
Moisture Vapor Transmission 0.394 cc-mm/m²-24hr-atm
1.00 cc-mil/100 in²-24hr-atm
ASTM E96
Melt Flow 11 g/10 min
11 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 20.7 MPa
3000 psi
ASTM D882
1% Secant Modulus 483 MPa
70000 psi
ASTM D882
Dart Drop 9.45 g/micron
240 g/mil
F50; ASTM D1709
Heat Seal Strength Initiation Temperature 124 °C
255 °F
Minimum seal strength is 200 g/in at 15 psi pressure and 1 sec.; ASTM D1709
Thermal Properties Metric English Comments
Melting Point 134 °C
273 °F
DSC-2 Differential Scanning Calorimeter
Optical Properties Metric English Comments
Haze 2.0 %
2.0 %
ASTM D1003
Gloss 85 %
85 %
45°; ASTM D2457