| Category | Metal , Nonferrous Metal , Nickel Alloy |
| Manufacturer | Weartech |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Weartech International WT-40 Nickel Hardfacing & Wear Resistant Alloy.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 8.30 g/cc | 0.300 lb/in³ |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell C | 35 - 45 | 35 - 45 | |
| Hardness, Vickers | 100 @Treatment Temp. 760 °C |
100 @Treatment Temp. 1400 °F |
|
| 220 @Treatment Temp. 649 °C |
220 @Treatment Temp. 1200 °F |
||
| 260 @Treatment Temp. 538 °C |
260 @Treatment Temp. 1000 °F |
||
| 350 @Treatment Temp. 427 °C |
350 @Treatment Temp. 800 °F |
||
| 420 @Treatment Temp. 25.0 °C |
420 @Treatment Temp. 77.0 °F |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 15.5 µm/m-°C | 8.60 µin/in-°F | |
| Specific Heat Capacity | 0.418 J/g-°C | 0.100 BTU/lb-°F | |
| Melting Point | <= 1010 °C | <= 1850 °F | |
| Liquidus | 1010 °C | 1850 °F |
| Component Elements Properties | Metric | English | Comments |
|---|---|---|---|
| Boron, B | 2.0 % | 2.0 % | |
| Carbon, C | 0.40 % | 0.40 % | |
| Chromium, Cr | 11 % | 11 % | |
| Iron, Fe | 2.0 % | 2.0 % | |
| Nickel, Ni | 82.4 % | 82.4 % | |
| Silicon, Si | 2.2 % | 2.2 % |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Relative Wear Performance | Cold Abrasion | Excellent |
| Corrosion | Excellent | |
| Erosion | Good/Moderate | |
| Hot Abrasion | Good/Moderate | |
| Impact | Not Recommended | |
| Metal to Metal | Excellent |