Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Universal Wire Works 132 Nickel Alloy Welding Wire

Category Metal , Nonferrous Metal , Nickel Alloy
Manufacturer Universal Wire Works
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Universal Wire Works 132 Nickel Alloy Welding Wire.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Alloy 132 is used for arc welding Inconel type alloy 600 and 601 and stainless alloy 330. Deposited weld metal has excellent high temperature strength and oxidation resistance. The dissimilar welding applications include joining Inconel and Incoloy type alloys to carbon steel, stainless steel, nickel and Monel type alloys; and joining carbon steels to Monel and stainless steels to carbon steel and nickel. Electrode sizes 3/32 and 1/8 diameter can be used in all positions, while the larger 5/32 and 3/16 diameters are used in the flat and horizontal positions. POWER SUPPLY DCRPInformation provided by Universal Wire Works for their line of welding wire and filler metal.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 552 MPa
80000 psi
Elongation at Break 30 %
30 %
Component Elements Properties Metric English Comments
Carbon, C <= 0.080 %
<= 0.080 %
Chromium, Cr 13 - 17 %
13 - 17 %
Cobalt, Co <= 0.12 %
<= 0.12 %
Copper, Cu <= 0.50 %
<= 0.50 %
Iron, Fe <= 11.5 %
<= 11.5 %
Manganese, Mn <= 3.5 %
<= 3.5 %
Nickel, Ni >= 62 %
>= 62 %
Niobium, Nb (Columbium, Cb) 1.5 - 4.0 %
1.5 - 4.0 %
Other <= 0.50 %
<= 0.50 %
Phosphorous, P <= 0.030 %
<= 0.030 %
Sulfur, S <= 0.020 %
<= 0.020 %
Tantalum, Ta <= 0.30 %
<= 0.30 %
Users viewing this material also viewed the following: