Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Trimay® Wear Plate TWP170 Flux Cored Weld Wire & Electrode

Category Metal , Nonferrous Metal , Nickel Alloy , Tungsten Alloy
Manufacturer Trimay® Wear Plate Ltd
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Trimay® Wear Plate TWP170 Flux Cored Weld Wire & Electrode.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Wire Description: TWP70 is a flux cored wire electrode for open-arc welding. Macrocrystalline tungsten carbide, nickel and boron fill a pure nickel tube which can be welded with or without shielding gas. Macrocrystalline tungsten has a higher melting point than that of the molten welding puddle, therefore the matrix is not affected by the degradation of Tunsten carbides throughout the matrix. The result is a stable matrix which is not brittle and can absorb impact without cracking.Key Performance Characteristics: Highest abrasion resistance, Highest impact resistance, Uniform carbide distribution throughout weld deposit, Crackless weld depositApplications:TWP70 can be applied on ferritic and austenitic steels using a open or closed arc welding procedure, with or without gas shielding. TWP70 is used to overlay and protect areas which are exposed to the most extreme abrasion and/or impact. TWP70 has been used for diamond bit augers, cement factory fan blades, bucket teeth, and crusher rolls.Information provided by Trimay®
Mechanical Properties Metric English Comments
Hardness, Rockwell C 48 - 50
48 - 50
Electrodes
50 - 55
50 - 55
Wire
Component Elements Properties Metric English Comments
Boron, B <= 5.0 %
<= 5.0 %
Nickel, Ni 30 - 50 %
30 - 50 %
WC 48 - 62 %
48 - 62 %
macrocrystalline
Descriptive Properties Value Comments
Available Sizes: Electrode 5
[mm]
6.4
[mm]
Available Sizes: Wire 1.6
[mm], cored wire
2.4
[mm], cored wire
2.8
[mm], cored wire
Packaging: Electrode 1
All Sizes- 5kg sleeves
Packaging: Wire 1
All Sizes- 25kg coils
Users viewing this material also viewed the following: