Tra-Con Tra-Cast 9182A Semi-Rigid Flame Retardant Epoxy Encapsulant

Category Polymer , Adhesive , Thermoset , Epoxy
Manufacturer Tra-Con, Inc.
Trade Name Tra-Cast
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tra-Con Tra-Cast 9182A Semi-Rigid Flame Retardant Epoxy Encapsulant.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
TRA-CAST 9182A is a medium viscosity, flame retardant epoxy encapsulant. It adheres well to most electronic and aerospace-industry materials like metals, glass, ceramic, industrial laminates and rigid plastics. TRA-CAST 9182A is recommended for potting, laminating, transformer encapsulating, filament winding and coil embedding applications where stress relief matched with fire retardancy is required. TRA-CAST 9182A has an easy mix ratio and is a durable electrical insulator, stable over a wide temperature range.Information provided by Tra-Con Inc.
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc
1.21 g/cc
Cured
Viscosity 35000 cP

@Temperature 25.0 °C
35000 cP

@Temperature 77.0 °F
After mixing
Mechanical Properties Metric English Comments
Hardness, Shore D 60
60
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 80.0 °C
176 °F
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
Dielectric Strength 15.7 kV/mm
400 kV/in
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature 90.0 °C
1.00 hour

@Temperature 194 °F
240 min

@Temperature 65.0 °C
4.00 hour

@Temperature 149 °F
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Descriptive Properties Value Comments
Color Black
Mix Ratio, parts by weight 100/100
Resin/Hardener
Working Life minutes 140