Teknor Apex Sinpolene GPP1615/2 Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 20% Glass Fiber Filler
Manufacturer Teknor Apex Company
Trade Name Sinpolene
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex Sinpolene GPP1615/2 Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Glass Fiber Reinforcement, 15% Filler by Weight Features: Good Dimensional Stability; High Heat Resistance; Good Impact Resistance; Medium Rigidity Uses: Automotive Applications; Housings; Pump Parts Appearance: Colors Available Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.16 g/cc
1.16 g/cc
ASTM D792
Linear Mold Shrinkage 0.0047 cm/cm
0.0047 in/in
ASTM D955
Linear Mold Shrinkage, Transverse 0.0047 cm/cm
0.0047 in/in
ASTM D955
Melt Flow 7.50 g/10 min

@Load 2.16 kg,
Temperature 230 °C
7.50 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 63.0 MPa
9140 psi
ASTM D638
Elongation at Break 11 %
11 %
ASTM D638
Flexural Strength 80.7 MPa
11700 psi
ASTM D790
Flexural Modulus 4.20 GPa
609 ksi
ASTM D790
Izod Impact, Notched 0.448 J/cm

@Temperature 22.8 °C
0.840 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 160 °C
320 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 149 °C

@Thickness 3.20 mm
300 °F

@Thickness 0.126 in
Unannealed; ASTM D648