Multibase 7-9600 Dow-Corning Soft Filling Elastomer Parts A and B

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Multibase
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase 7-9600 Dow-Corning Soft Filling Elastomer Parts A and B.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Multibase
Physical Properties Metric English Comments
Viscosity 400 cP
400 cP
Part A
400 cP
400 cP
Part B
Mechanical Properties Metric English Comments
Penetration 245 - 275
245 - 275
mm/10, after cure