| Category | Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) |
| Manufacturer | Techmer ES |
| Trade Name | HiFill® |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Techmer ES HiFill® PPS 0334 A.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 3.44 g/cc | 0.124 lb/in³ | ASTM D792 |
| Water Absorption | 0.020 % @Time 86400 sec |
0.020 % @Time 24.0 hour |
ASTM D570 |
| Linear Mold Shrinkage, Flow | 0.0030 cm/cm @Thickness 3.17 mm |
0.0030 in/in @Thickness 0.125 in |
ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 100 | 100 | ASTM D785 |
| Tensile Strength, Yield | 89.6 MPa | 13000 psi | ASTM D638 |
| Elongation at Break | 1.0 % | 1.0 % | ASTM D638 |
| Flexural Strength | 138 MPa | 20000 psi | ASTM D790 |
| Flexural Modulus | 12.4 GPa | 1800 ksi | ASTM D790 |
| Izod Impact, Notched | 0.374 J/cm @Thickness 3.17 mm |
0.700 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
| Thermal Conductivity | 1.73 W/m-K | 12.0 BTU-in/hr-ft²-°F | ASTM C177 |
| Deflection Temperature at 0.46 MPa (66 psi) | 280 °C | 536 °F | Unannealed; ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 266 °C | 510 °F | Unannealed; ASTM D648 |
| UL RTI, Electrical | 220 °C @Thickness 1.50 mm |
428 °F @Thickness 0.0591 in |
UL746 |
| Flammability, UL94 | V-0 | V-0 | |
| 5VB | 5VB |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 10000 - 1.00e+6 ohm-cm | 10000 - 1.00e+6 ohm-cm | ASTM D257 |