Mechanical Properties Metric English Comments
Tensile Strength, Yield 89.6 MPa
13000 psi
Type I, 5.1 mm/min; ASTM D638
PolyOne Gravi-Tech™ GRV-NY-035-SS-GF-BLK Polyamide 6 (Nylon 6)
Information provided by PolyOne
Tensile Strength, Yield 89.6 MPa
13000 psi
ASTM D638
Omni Plastics OmniLon™ 6/6 PA6/6 HSL Unfilled/ Impact Modified Nylon
Applications: Structural and appearance parts across industry segments including automotive, heavy truck fans, appliances, furniture, lawn and garden.Information provided by Omni Plastics
Tensile Strength, Yield 89.6 MPa

@Thickness 3.17 mm
13000 psi

@Thickness 0.125 in
Nilit Polynil® N66-P50N Lubed Nylon 6/6
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Tensile Strength, Yield 89.6 MPa
13000 psi
PSM Industries Pacific Sintered Metals Iron F-200-P Powdered Metal
Low stressed mechanical components, Soft magnetic applications Equivalent MPIF Specification: F-0000-10Information Provided by Pacific Sintered Metals, a division of PSM Industries
Tensile Strength, Yield 89.6 MPa

@Temperature 23.9 °C
13000 psi

@Temperature 75.0 °F
0° Direction, Dry; 325°F, 1000psi Cured; ASTM D638
Park Electrochemical Nelcote® F-502 Phenolic Prepreg, Silica Reinforced
Nelcote® F-502 is a MIL-R-9299 phenolic resin system suitable for impregnation on any MIL-C-9084 fabric with a compatible finish. F-502 is used in the manufacture of ablative reinforcements in rock..
Tensile Strength, Yield 89.6 MPa
13000 psi
ASTM D638
Polymer Resources TP-FRG15 Polybutylene Terephthalate, 15% Glass Reinforced, Flame Retardant
Polybutylene Terephthalate, 15% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples..
Tensile Strength, Yield 89.6 MPa
13000 psi
ASTM D638
Polymer Resources TP-G15 Polybutylene Terephthalate, 15% Glass Reinforced
Polybutylene Terephthalate, 15% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information prov..
Tensile Strength, Yield 89.6 MPa
13000 psi
ASTM D638
Polymer Resources NY66-GP2 General Purpose Nylon 66, Nucleated
General Purpose Nylon 66, Nucleated Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry..
Tensile Strength, Yield 89.6 MPa
13000 psi
ASTM D638
Polymer Resources NY6-GP2-[color]-H General Purpose Nylon 6, Nucleated, Heat Stabilized
General Purpose Nylon 6, Nucleated, Heat StabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades..
Tensile Strength, Yield 89.6 MPa
13000 psi
ASTM D638
Polymer Resources NY6-M40 Nylon 6, 40% Mineral Filled
Nylon 6, 40% Mineral Filled, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested ..
Tensile Strength, Yield 89.6 MPa
13000 psi
ASTM D638
Polymer Resources NY6-M40-[color]-H Nylon 6, 40% Mineral Filled, Heat Stabilized
Nylon 6, 40% Mineral Filled, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon g..
Tensile Strength, Yield 89.6 MPa
13000 psi
ASTM D638
Ravago Manufacturing Americas Hylon® N2040ML Nylon 6 (DAM)
Information provided by Ravago.
Tensile Strength, Yield 89.6 MPa
13000 psi
ASTM D638
Fiberfil® J-60/30/E/HF Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled, improved flow
Information provided by FIBERFIL Engineered Plastics
Tensile Strength, Yield 89.6 MPa

@Thickness 3.17 mm
13000 psi

@Thickness 0.125 in
LW
Industrial Laminates/Norplex MC330 Cotton Fabric
Description: Grade MC330 is a cotton cloth/phenolic resin composite which is specially processed to be used in cryogenic applications. Such applications include spacers for installation of liquid ox..
Tensile Strength, Yield 89.6 MPa
13000 psi
ASTM D638
Techmer ES Elastoblend® PA6 GF15 IM L 15% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impac..
Tensile Strength, Yield 89.6 MPa
13000 psi
ASTM D638
Techmer ES HiFill FR® PA6/6 GF10 FR HS BK 10% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 10% Filler by WeightAdditive: Heat StabilizerFeatures: Flame Retardant and Heat StabilizedAppearance: BlackTPCI# 9550101In..
Tensile Strength, Yield 89.6 MPa
13000 psi
ASTM D638
Techmer ES HiFill® PA6 0135 BL069 13% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 13% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedAppearanc..
Tensile Strength, Yield 89.6 MPa
13000 psi
ASTM D638
Spartech PP5440 Glass Fiber Reinforced Homopolymer
Provides the maximum strength and heat resistance among polypropylene compounds. Physical properties can approach those of more expensive engineering resins.Information provided by Spartech
Tensile Strength, Yield 89.6 MPa
13000 psi
ASTM D638
Techmer ES HiFill® PA6 GF/B20 A2 20% Glass Fiber/Glass Bead Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber/Glass Bead, 20% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedInformation ..
Tensile Strength, Yield 89.6 MPa
13000 psi
ASTM D638
Techmer ES HiFill® POM CO GF10 CC 10% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforced, 10% Filler by WeightFeatures: Copolymer and Chemically CoupledInformation provided by TP Composites, Inc.
Tensile Strength, Yield 89.6 MPa
13000 psi
ASTM D638
Techmer ES Luriblend® PA6 ML2 Nylon 6
Availability: North AmericaForms: PelletsAdditive: Molybdenum Disulfide Lubricant(2%)Features: Good Wear Resistance, Low Friction and LubricatedInformation provided by TP Composites, Inc.
Tensile Strength, Yield 89.6 MPa
13000 psi
ASTM D638
Techmer ES Statiblend® PA6 GF20 AS BK 20% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 20% Filler by WeightAdditive: Antistatic, Heat Stabilizer and LubricantFeatures: Antistatic, Heat Stabilizer and Lubricate..
Tensile Strength, Yield 89.6 MPa
13000 psi
ASTM D638
Techmer ES HiFill FR® PA6 GF13 FR-N IM BK 13% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 13% Filler by WeightAdditive: Heat Stabilize, Impact Modifier and LubricantFeatures: Flame Retardant, Heat S..
Tensile Strength, Yield 89.6 MPa
13000 psi
ASTM D638
Techmer ES HiFill® PPS 0334 A
Availability: North AmericaForms: PelletsFeatures: High DensityInformation provided by TP Composites, Inc.
Tensile Strength, Yield 89.6 MPa
13000 psi
ISO 527
Westlake Plastics MediPEEK IM Polyetheretherketone for Medical Applications
MediPEEK-IM is a high performance semi-crystalline thermoplastic designed for long term body contact as an implantable material. It is USP Class VI and compliant to ASTM F2026. It has excellent st..
Tensile Strength, Yield 89.6 - 152 MPa
13000 - 22000 psi
0.2% offset
Eagle Brass 425 Tin Brass 2%, Annealed
Alloy C425 is a low zinc-containing alloy with good combination of tensile strength, electrical conductivity, formability and corrosion resistance. Applications include electrical springs, connector..
Tensile Strength, Yield 89.6 - 172 MPa
13000 - 25000 psi
0.2% offset
Eagle Brass 706 Copper Nickel 10%, Annealed
706 exhibits excellent corrosion resistance, especially in marine applications. It has a relatively high strength and has resistance at elevated temperatures. The cost is relatively high compared to..
Tensile Strength, Yield 89.6 MPa
13000 psi
ASTM D638
Clariant Renol PA123G13 Nylon 66, 13% Glass Fiber, Impact Modified, Heat Stabilized, Lubricated
Data provided by Clariant Masterbatches
Tensile Strength, Yield 89.6 MPa
13000 psi
Type 1 - Rigids, Break, 0.2 in/min; ASTM D638
PolyOne Edgetek® NL-10GF/000 Nylon 6/12, Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedInformation provided by PolyOne Corporation.
Tensile Strength, Yield 89.6 MPa
13000 psi
ASTM D638
Techmer ES HiFill FR® PPO/HIPS GF20 BK 20% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 20% Filler by Weight Appearance: BlackInformation provided by TP Composites, Inc.