| Category | Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 30% Glass Fiber Filled | 
| Manufacturer | Techmer ES | 
| Trade Name | HiFill® | 
| Port | Shanghai port,China | 
| Trade Terms | FOB, CFR, CIF | 
| Payment Terms | L/C, T/T, Western Union | 
| Download PDF | Techmer ES HiFill® PA6 GF30 L X MT 30% Glass Filled.pdf  | 
          
| Price | EMAIL US sales@lookpolymers.com | 
| Physical Properties | Metric | English | Comments | 
|---|---|---|---|
| Density | 1.36 g/cc | 0.0491 lb/in³ | ASTM D792 | 
| Water Absorption |           1.1 %                     @Time 86400 sec  | 
                  1.1 %                     @Time 24.0 hour  | 
        ASTM D570 | 
| Linear Mold Shrinkage, Flow |           0.0030           cm/cm           @Thickness 3.17 mm  | 
                  0.0030           in/in           @Thickness 0.125 in  | 
        ASTM D955 | 
| Mechanical Properties | Metric | English | Comments | 
|---|---|---|---|
| Hardness, Rockwell R | 118 | 118 | ASTM D785 | 
| Tensile Strength, Yield | 162 MPa | 23500 psi | ASTM D638 | 
| Elongation at Break | 2.4 % | 2.4 % | ASTM D638 | 
| Flexural Strength | 255 MPa | 37000 psi | ASTM D790 | 
| Flexural Modulus | 8.27 GPa | 1200 ksi | ASTM D790 | 
| Izod Impact, Notched |           1.28           J/cm           @Thickness 3.17 mm  | 
                  2.40           ft-lb/in           @Thickness 0.125 in  | 
        ASTM D256 | 
| Thermal Properties | Metric | English | Comments | 
|---|---|---|---|
| CTE, linear, Parallel to Flow | 21.6 µm/m-°C | 12.0 µin/in-°F | ASTM D696 | 
| Deflection Temperature at 0.46 MPa (66 psi) | 216 °C | 420 °F | Unannealed; ASTM D648 | 
| Deflection Temperature at 1.8 MPa (264 psi) | 207 °C | 405 °F | Unannealed; ASTM D648 | 
| Electrical Properties | Metric | English | Comments | 
|---|---|---|---|
| Volume Resistivity | 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | ASTM D257 | 
| Dielectric Strength | 16.1 kV/mm | 410 kV/in | Method A (Short-Time); ASTM D149 |