| Category | Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Impact Modified |
| Manufacturer | Techmer ES |
| Trade Name | HiFill FR® |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Techmer ES HiFill FR® HIPS FR V-2.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.14 g/cc | 0.0412 lb/in³ | ASTM D792 |
| Water Absorption | 0.050 % @Time 86400 sec |
0.050 % @Time 24.0 hour |
ASTM D570 |
| Linear Mold Shrinkage, Flow | 0.045 cm/cm @Thickness 3.17 mm |
0.045 in/in @Thickness 0.125 in |
ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell L | 60 | 60 | ASTM D785 |
| Tensile Strength, Yield | 20.7 MPa | 3000 psi | ASTM D638 |
| Elongation at Break | 30 % | 30 % | ASTM D638 |
| Flexural Strength | 27.6 MPa | 4000 psi | ASTM D790 |
| Flexural Modulus | 1.93 GPa | 280 ksi | ASTM D790 |
| Izod Impact, Notched | 0.908 J/cm @Thickness 3.17 mm |
1.70 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
| Izod Impact, Unnotched | >= 4.27 J/cm @Thickness 3.17 mm |
>= 8.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 63.0 µm/m-°C | 35.0 µin/in-°F | ASTM D696 |
| Deflection Temperature at 0.46 MPa (66 psi) | 96.1 °C | 205 °F | Unannealed; ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 87.8 °C | 190 °F | Unannealed; ASTM D648 |
| Flammability, UL94 | V-2 | V-2 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | ASTM D257 |
| Dielectric Strength | 21.7 kV/mm | 550 kV/in | Method A (Short-Time); ASTM D149 |