| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Strength | 27.6 MPa | 4000 psi | ASTM D790 |
|
Multibase Multi-Pro® 1510 CNU White Polypropylene
Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
|
|||
| Flexural Strength | 27.6 MPa | 4000 psi | ASTM D790 |
|
Oxford Polymers PC 20 Unfilled Polycarbonate for Injection Molding
Unfilled Polycarbonate for Injection MoldingInformation provided by Oxford Polymers.
|
|||
| Flexural Strength | 27.6 MPa | 4000 psi | ASTM D790 |
|
Niche Polymer PPCM10BK Copolymer PP
Information provided by Niche Polymer
|
|||
| Flexural Strength | 27.6 MPa | 4000 psi | ASTM D790 |
|
Niche Polymer PPCM15BK Copolymer PP
Information provided by Niche Polymer
|
|||
| Flexural Strength | 27.6 MPa | 4000 psi | |
|
Pyrotek ISOMAG® 175 Structural Insulation Board
Isomag® 70 is a high strength insulating board suitable as an electrical insulator or a thermal barrier material in a variety of industrial applications. Its magnesia silicate based formulation pr..
|
|||
| Flexural Strength | 27.6 MPa | 4000 psi | ASTM D790 |
|
Quadrant EPP Fluorosint® MT-01 Proprietary fluoropolymer reinforced with carbon fibers and organometallic fillers( ASTM Product Data Sheet) |
|||
| Flexural Strength | 27.6 MPa | 4000 psi | ASTM D790 |
|
Network Polymers 707 Polystyrene
Description: Ignition RetardantInformation provided by Network Polymers Inc.
|
|||
| Flexural Strength | 27.6 MPa | 4000 psi | ASTM D790 |
|
Ravago Manufacturing Americas Hylon® N1000STHL Nylon 6/6 (Cond)
Information provided by Ravago
|
|||
| Flexural Strength | 27.6 MPa | 4000 psi | ASTM D790 |
|
Quadrant EPP Fluorosint® MT-01 Enhanced PTFE (ASTM Product Data Sheet)
(Unverified Data**) |
|||
| Flexural Strength | 27.6 MPa | 4000 psi | Conditioned; ASTM D790 |
|
Ravago Manufacturing Americas Hylon® N1000STHL UV2 Nylon 6/6
(discontinued **)
Available in North America Additive: Heat Stabilizer, Lubricant and UV StabilizerFeatures: Good Toughness, Lubricated, Heat StabilizedRoHS CompliantAuto Specifications: GM GMP.PA66.074 Color: BlackF..
|
|||
| Flexural Strength | 27.6 MPa | 4000 psi | ASTM D790 |
|
I. Stern 550 High Impact Polystyrene
Features:Good process propertiesExcellent toughness and environmental stress crackingApplicationsStructural foamDisplaysSmall appliancesAgency RatingsFDA Title 21 CFR 177.1640UL File E220962Informat..
|
|||
| Flexural Strength | 27.6 MPa | 4000 psi | ASTM D790 |
|
Techmer ES Statiblend® 02010 MB Polypropylene
Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified FillerReinfor.Features: ConductiveAppearance: BlackTPCI# 9125116Information provided by TP Composites, Inc.
|
|||
| Flexural Strength | 27.6 MPa | 4000 psi | ASTM D790 |
|
Teknor Apex Chemlon® 275H Nylon 6, Copolymer, Impact Modified
Notes: Very high impact and elongation, low flexural modulus material for tubing and wire jacketing applications requiring a soft, flexible product; FMVSS Flammability: Passes, FMVSS 302Processing M..
|
|||
| Flexural Strength | 27.6 MPa | 4000 psi | ASTM D790 |
|
Techmer ES HiFill FR® HIPS FR V-2
Availability: North AmericaForms: PelletsFeatures: Flame RetardantInformation provided by TP Composites, Inc.
|
|||
| Flexural Strength | 27.6 MPa | 4000 psi | ASTM D790 |
|
Chase Plastics CP Pryme® N100STL (COND, 50% RH) Nylon 6, Super Toughened, Internally Lubricated
Information provided by Chase Plastics.
|
|||
| Flexural Strength | 27.6 MPa | 4000 psi | ASTM D790 |
|
Westlake Plastics Propylux® CN-P Polypropylene (conductive)
Carbon-powder-filled lightweight material with good chemical resistance, extremely low water absorption level, and high impact resistance (no break, notched or unnotched). Rated UL94 V-0.Informatio..
|
|||
| Flexural Strength | 27.6 MPa | 4000 psi | ASTM D790 |
|
Eastman Tenite 285A2R30020 Cellulose Acetate Butyrate, Natural, Trsp
Applications:Tool handlesToys/sporting goodsProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clar..
|
|||
| Flexural Strength | 27.6 MPa | 4000 psi | ASTM D790 |
|
Chesterton MRS S4+ Metal Rebuilding System
An advanced polymer composite formulated to protect equipment from extreme chemical attack and corrosion. It is typically applied by spray, roller or brush at a nominal thickness of 375 microns (15 ..
|
|||
| Flexural Strength | 27.6 MPa | 4000 psi | ASTM D790 |
|
CPC - Vycom SEABOARD™ LITE High density polyethylene (HDPE)
Seaboard Lite is a high density polyethylene (HDPE) sheet formulated to meet the specific requirements of marine and other outdoor environments. Seaboard Lite is UV stable and will withstand the ele..
|
|||
| Flexural Strength | 27.6 MPa | 4000 psi | |
|
Abatron ROCKWELD 55-27 A/B Structural Adhesive Putty; Epoxy
ROCKWELD 55-27 is a 2-component epoxy system with low density, high-strength, and no shrinkage. It is a structural adhesive putty for sculpturing, repairs and restoration of stone, concrete and maso..
|
|||
| Flexural Strength | 27.6 MPa | 4000 psi | |
|
Aremco AREMCOLOX™ 502-1400 (Bisque-fired) Machinable Alumina
Good corrosion electrical and thermal shock resistance. Plates from 1/4" to 3/4" thick; rods from 1/4" to 3" diameter. Easily machined using conventional tools, no firing required.
|
|||
| Flexural Strength |
27.6
MPa <br>@Temperature 150 °C
|
4000
psi <br>@Temperature 302 °F
|
ISO 178 |
|
Solvay Specialty Polymers Amodel® A-1240 L Polyphthalamide (PPA)
(discontinued **)
Amodel A-1240 L is a 40% mineral filled polyphthalamide (PPA) that offers low warpage and excellent dimensional stability. This resin also has a high deflection temperature, flexural modulus and ten..
|
|||
| Flexural Strength | 27.6 MPa | 4000 psi | ASTM D790 |
|
Chesterton ARC S4+ 100% Novolac acid resistant coating
Description: An advanced polymer composite formulated to protect equipment from extreme chemical attack and corrosion. It is typically applied by spray, roller or brush at a nominal thickness of 375..
|
|||