Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Styron Magnumâ„¢ 2645 ABS, Impact Grade

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded
Manufacturer Styron
Trade Name Magnum™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Styron Magnumâ„¢ 2645 ABS, Impact Grade.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ABS resin are available in a wide range of melt flow rates, impact strength and heat resistance for both high and low gloss applications manufactured by injection molding, sheet or profile extrusion and thermoforming.The 2600 series of MAGNUM ABS resins are designated for use in healthcare applications. Both high and low gloss resins are available which have passed the USP XXIII Class IV medical testing. Other non-USP classified testing is also done on the MAGNUM 2600 series of ABS resins to evaluate the biocompatibility of the resins.MAGNUM 2645 ABS resin is a higher impact strength version of the low gloss MAGNUM 2642. With an Izod impact strength of 290 J/m, it is applicable to those low gloss applications needing a moderate amount of impact strength while maintaining its processability.Data provided by Dow Chemical.This product line was spun off from Dow Chemical to Styron in 2010.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ASTM Data
Linear Mold Shrinkage 0.0055 cm/cm
0.0055 in/in
Melt Flow 6.0 g/10 min

@Load 3.80 kg,
Temperature 230 °C
6.0 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM Data
Mechanical Properties Metric English Comments
Hardness, Rockwell R 104
104
Tensile Strength, Yield 44.8 MPa
6500 psi
ASTM Data
Elongation at Yield 2.5 %
2.5 %
ISO Data
Tensile Modulus 2.21 GPa
321 ksi
ASTM Data
Izod Impact, Notched 2.88 J/cm
5.40 ft-lb/in
ASTM Data
Charpy Impact Unnotched 8.00 J/cm²
38.1 ft-lb/in²
ISO Data, Low Temp
NB
NB
ISO Data
Charpy Impact, Notched 0.800 J/cm²
3.81 ft-lb/in²
ISO Data, Low Temp
2.40 J/cm²
11.4 ft-lb/in²
ISO Data
Impact Test 51.0 J

@Temperature 23.0 °C
37.6 ft-lb

@Temperature 73.4 °F
Instrumented Dart Total Energy
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 102 µm/m-°C

@Temperature 20.0 °C
56.7 µin/in-°F

@Temperature 68.0 °F
ISO data
Deflection Temperature at 0.46 MPa (66 psi) 93.0 °C
199 °F
Unannealed; ASTM Data
Deflection Temperature at 1.8 MPa (264 psi) 79.0 °C
174 °F
Unannealed; ASTM Data
96.1 °C
205 °F
Annealed; ASTM Data
Vicat Softening Point 104 °C
219 °F
Optical Properties Metric English Comments
Gloss 52.5 %
52.5 %
Gardner Gloss, 60°
Users viewing this material also viewed the following: