| Category | Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Impact Modified |
| Manufacturer | Styrolution |
| Trade Name | PS |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Styrolution PS 5300 HIPS.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.04 g/cc | 0.0376 lb/in³ | ASTM D 792 |
| Linear Mold Shrinkage | 0.0040 - 0.0070 cm/cm | 0.0040 - 0.0070 in/in | ASTM D 955 |
| Melt Flow | 2.6 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.6 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D 1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell L | 45 | 45 | ASTM D 785 |
| Tensile Strength, Yield | 17.7 MPa | 2560 psi | ASTM D 638 |
| Elongation at Break | 53 % | 53 % | ASTM D 638 |
| Tensile Modulus | 1.79 GPa | 260 ksi | ASTM D 638 |
| Flexural Strength | 41.4 MPa | 6000 psi | ASTM D 790 |
| Flexural Modulus | 1.72 GPa | 250 ksi | ASTM D 790 |
| Izod Impact, Notched | 1.17 J/cm | 2.20 ft-lb/in | ASTM D 638 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 90.0 µm/m-°C | 50.0 µin/in-°F | ASTM D 696 |
| Vicat Softening Point | 101 °C @Load 1.02 kg |
214 °F @Load 2.25 lb |
120°C/h; ASTM D 1525 |
| Flammability, UL94 | HB | HB |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Gloss | 15 % | 15 % | Specular Gloss, 60°; ASTM D 523 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Constant | 2.5 @Thickness 1.00 mm, Frequency 1.00e+6 Hz |
2.5 @Thickness 0.0394 in, Frequency 1.00e+6 Hz |
ASTM D 150 |
| Dielectric Strength | 15.7 kV/mm | 400 kV/in | ASTM D 696 |