Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Omnix® 9050 Polyamide, High Performance (HPPA), 50% Glass Fiber

Category Polymer , Thermoplastic , Nylon
Manufacturer Solvay Specialty Polymers
Trade Name Omnix®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Omnix® 9050 Polyamide, High Performance (HPPA), 50% Glass Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Omnix® 9050 is a 50% glass-fiber reinforced high-performance polyamide. It is hot-water moldable and intended for use in components requiring superior mechanical properties even after moisture absorption.Omnix® 9050 is characterized by high stiffness and strength, very good impact properties, good dimensional stability and high flow properties. This material is an economical alternative to die-cast alloys for application in automotive, electrical appliance and mechanical equipment. It processes readily using conventional injection molding machines and methods. Water-cooled molds are suitable for use with this grade. Features: Fast Molding Cycle; Good Dimensional Stability; Good Impact Resistance; Good Surface Finish; High Flow; High Stiffness; High Strength; Hot Water Moldability; PaintableUses: Automotive Applications; Electrical/Electronic Applications; Machinery Maintenance/RepairInformation provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.60 g/cc
0.0578 lb/in³
ASTM D792
Filler Content 50 %
50 %
Glass Fiber
Water Absorption 0.27 %

@Time 86400 sec
0.27 %

@Time 24.0 hour
ISO 62
Linear Mold Shrinkage, Flow 0.0020 cm/cm
0.0020 in/in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.0050 cm/cm
0.0050 in/in
ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength, Yield 235 MPa
34100 psi
ISO 527-2
Elongation at Break 2.1 %
2.1 %
ISO 527-2
Tensile Modulus 17.0 GPa
2470 ksi
ISO 527-2
Flexural Strength 340 MPa
49300 psi
ISO 178
Flexural Modulus 15.0 GPa
2180 ksi
ISO 178
Izod Impact, Notched (ISO) 13.0 kJ/m²
6.19 ft-lb/in²
Type 1, Notch A; ISO 180
Izod Impact, Unnotched (ISO) 75.0 kJ/m²
35.7 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
ISO 11357-3
Deflection Temperature at 1.8 MPa (264 psi) 248 °C
478 °F
Unannealed; ISO 75-2/A
Flammability, UL94 HB
HB
Processing Properties Metric English Comments
Rear Barrel Temperature 250 °C
482 °F
Front Barrel Temperature 285 °C
545 °F
Melt Temperature 275 - 290 °C
527 - 554 °F
Mold Temperature 80.0 - 120 °C
176 - 248 °F
Drying Temperature 80.0 °C

@Time 14400 - 43200 sec
176 °F

@Time 4.00 - 12.0 hour
Descriptive Properties Value Comments
Availability Asia Pacific
Europe
North America
Color Black; Natural
Form Pellets
Part Marking Code >PAMXD6/66-GF50<
ISO 11469
Processing Technique Injection Molding; Water-Heated Mold Injection Molding
RoHS Compliance RoHS Compliant
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved