Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Engineered Polymers DEXPRO® R210 TPV - High-Impact Polypropylene  (discontinued **)

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Vulcanizate Elastomer (TPV) , Polypropylene (PP)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Engineered Polymers DEXPRO® R210 TPV - High-Impact Polypropylene  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: DEXPRO® R210 is a high-impact polypropylene co-polymer molding compound. Applications: Exterior trimInformation provided by Solvay Engineered Polymers. LyondellBasell acquired Solvay Engineered Polymers in 2008. This grade is not part of the current LyondellBasell product line.
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ISO 1183
Linear Mold Shrinkage 0.013 - 0.016 cm/cm
0.013 - 0.016 in/in
as molded; ISO 294
0.017 - 0.020 cm/cm
0.017 - 0.020 in/in
after bake; ISO 294
Melt Flow 12 g/10 min
12 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 17.5 MPa
2540 psi
150x10x4 mm specimen, 50 mm/min; ISO 527-1/527-2
Flexural Modulus 0.715 GPa
104 ksi
80x10x4 mm specimen, 2 mm/min; ISO 178
Thermal Properties Metric English Comments
CTE, linear 105 µm/m-°C

@Temperature -30.0 - 80.0 °C
58.3 µin/in-°F

@Temperature -22.0 - 176 °F
ASTM E228