SABIC M200056 High Density Polyethylene for Injection Molding

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer SABIC
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC M200056 High Density Polyethylene for Injection Molding.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Product Description: M200056 is a high density polyethylene grade with a narrow molecular weight distribution suitable for injection molding applications. It has been designed to provide good flow properties, low warpage with good dimensional stability and high gloss.Typical Applications: M200056 is recommended for housewares, food containers, toys, caps and closures, etc.Information provided by SABIC.
Physical Properties Metric English Comments
Density 0.956 g/cc
0.0345 lb/in³
ASTM D1505
ESCR 100% Igepal® 3.0 hour
3.0 hour
F50; ASTM D1693B
ESCR 10% Igepal® 2.0 hour
2.0 hour
F50; ASTM D1693B
Melt Flow 20 g/10 min

@Load 2.16 kg,
Temperature 190 °C
20 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 60
60
ASTM D2240
Tensile Strength at Break 12.0 MPa
1740 psi
ASTM D638
Tensile Strength, Yield 24.0 MPa
3480 psi
ASTM D638
Elongation at Break >= 200 %
>= 200 %
ASTM D638
Flexural Strength 23.0 MPa
3340 psi
ASTM D790
Flexural Modulus 0.825 GPa
120 ksi
ASTM D790
1% Secant Modulus 800 MPa
116000 psi
ASTM D638
Izod Impact, Notched 0.300 J/cm
0.562 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Vicat Softening Point 124 °C
255 °F
ASTM D1525
Brittleness Temperature <= -75.0 °C
<= -103 °F
ASTM D746
Processing Properties Metric English Comments
Mold Temperature 15.0 - 60.0 °C
59.0 - 140 °F
Injection Pressure 60.0 - 100 MPa
8700 - 14500 psi