Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | <= -75.0 °C | <= -103 °F | ASTM D746 |
SABIC MG200024 Linear Low Density Polyethylene for Compounding Product Description: MG200024 is a Linear Low Density Polyethylene grade with a narrow molecular weight distribution primarily suitable for compounding. It is in the powder form designed to give g.. |
|||
Brittleness Temperature | <= -75.0 °C | <= -103 °F | ASTM D746 |
Polimeri Europa Riblene® FC 30 Low Density Polyethylene - Blown Film Extrusion Riblene FC 30 is a high molecular weight low density polyethylene resin (LDPE) suitable for blown film extrusion. Riblene FC 30 is characterized by a high melt strength leading to a good bubble sta.. |
|||
Brittleness Temperature | <= -75.0 °C | <= -103 °F | ASTM D746 |
Polimeri Europa Riblene® FC 40 Low Density Polyethylene - Blown Film Extrusion Riblene FC 40 is a high molecular weight low density polyethylene (LDPE) suitable for blown film extrusion. Riblene FC 40 is characterized by a high melt strength leading to a good bubble stability.. |
|||
Brittleness Temperature | <= -75.0 °C | <= -103 °F | ASTM D746 |
Polimeri Europa Riblene® FF 34 Low Density Polyethylene - Blown Film Extrusion Riblene FF 34 is a high molecular weight low density polyethylene (LDPE), with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FF 34 is characterized by a good melt s.. |
|||
Brittleness Temperature | <= -75.0 °C | <= -103 °F | ASTM D746 |
SABIC M80064 Series High Density Polyethylene for Injection Molding Product Description: M80064 is a high density polyethylene grade with a narrow molecular weight distribution suitable for injection molding applications. It has been designed to provide good rigid.. |
|||
Brittleness Temperature | <= -75.0 °C | <= -103 °F | ASTM D746 |
SABIC R50035 Linear Low Density Polyethylene for Rotational Molding Product Description: R50035 are Linear Low Density Polyethylene grades designed to provide excellent stress crack resistance, mechanical properties with high rigidity, toughness, gloss and low warp.. |
|||
Brittleness Temperature | <= -75.0 °C | <= -103 °F | ASTM D746 |
Chevron Phillips HiD® 9402 HDPE Blow Molding Resin
(discontinued **) Resin Type: Linear Homopolymer; Blow Molding, Sheeting and Profile ResinCharacteristics: High Melt Strength - Larger Parts, Wide Range of Processing Conditions, High Stiffness and Impact Resistance,.. |
|||
Brittleness Temperature | <= -75.0 °C | <= -103 °F | Type A, type 1 specimen; ASTM D746 |
Chevron Phillips Marlex® C513UV HDPE Blow Molding Resin
(discontinued **) Resin Type: Hexene CopolymerCharacteristics: Outstanding impact resistanceExcellent ESCRExcellent processabilityUV stabilizationApplications: Intermediate bulk containersAgricultural containersInfor.. |
|||
Brittleness Temperature | <= -75.0 °C | <= -103 °F | ASTM D746 |
Ineos B54-25H-127 HDPE B54-25H-127 is a high density polyethylene copolymer developed for blow molding. It is recommended for use in applications which require a combination of high top load strength and good environmenta.. |
|||
Brittleness Temperature | <= -75.0 °C | <= -103 °F | ASTM D746 |
Ineos G36-24-150 HDPE Ineos G36-24-150 is a medium density polyethylene resin designed for geomembrane sheet extrusion. The resin has excellent environmental stress crack resistance (ESCR).Natural resin; some physical p.. |
|||
Brittleness Temperature | <= -75.0 °C | <= -103 °F | ASTM D 746 |
Ineos HP55-25-155 HDPE A high performance high density polyethylene copolymer developed for blow molding. It is recommended for use in continuous extrusion blowmolding equipment, specifically where applications require ex.. |
|||
Brittleness Temperature | <= -75.0 °C | <= -103 °F | ASTM D746 |
Ineos T50-4400 HDPE Ineos T50-4400 is a high-flow high density polyethylene copolymer intended for injection molding of thin wall containers. This material will allow for cycle time reduction while still imparting rea.. |
|||
Brittleness Temperature | <= -75.0 °C | <= -103 °F | F<sub>50</sub>; ASTM D746 |
LyondellBasell Alathon® L5040TC High Density Polyethylene ApplicationsALATHON L 5040TC is a bimodal high density polyethylene copolymer natural resin designed for telecommunications conduits. L 5040TC offers an excellent balance of stiffness, toughness and.. |
|||
Brittleness Temperature | <= -75.0 °C | <= -103 °F | ASTM D746 |
Ineos K44-11-128 HDPE Ineos K44-11-128 is a high molecular weight, high density polyethylene copolymer intended for large part blow molding where the finished product demands good physical performance and low color. Thi.. |
|||
Brittleness Temperature | <= -75.0 °C | <= -103 °F | ASTM D746 |
UBE F320 Polyethylene Description: UBE Polyethylene is polymerized at high pressure using a tubular reactor. Production conditions are strictly controlled ensuring the product's superior physical and mechanical prope.. |
|||
Brittleness Temperature | <= -75.0 °C | <= -103 °F | ASTM D746 |
UBE F522N Polyethylene Description: UBE Polyethylene is polymerized at high pressure using a tubular reactor. Production conditions are strictly controlled ensuring the product's superior physical and mechanical prope.. |
|||
Brittleness Temperature | <= -75.0 °C | <= -103 °F | ASTM D746 |
UBE R500 Polyethylene Description: UBE Polyethylene is polymerized at high pressure using a tubular reactor. Production conditions are strictly controlled ensuring the product's superior physical and mechanical prope.. |
|||
Brittleness Temperature | <= -75.0 °C | <= -103 °F | ASTM D746 |
UBE B028 Polyethylene Description: UBE Polyethylene is polymerized at high pressure using a tubular reactor. Production conditions are strictly controlled ensuring the product's superior physical and mechanical prope.. |
|||
Brittleness Temperature | <= -75.0 °C | <= -103 °F | ASTM D746 |
UBE F019 Polyethylene Description: UBE Polyethylene is polymerized at high pressure using a tubular reactor. Production conditions are strictly controlled ensuring the product's superior physical and mechanical prope.. |
|||
Brittleness Temperature | <= -75.0 °C | <= -103 °F | ASTM D746 |
Chevron Phillips Marlex® 9505H High Density Polyethylene This gas phase, high molecular weight, hexene copolymer with antistatic agent is tailored for lightweight blow molded containers that:Require outstanding ESCRRequire excellent impact resistanceAre d.. |
|||
Brittleness Temperature | <= -75.0 °C | <= -103 °F | Type A, Type I specimen; ASTM D-746 |
Chevron Phillips Marlex® HHM TR-232 Polyethylene; Enhanced Low density linear polyethylene. This low density, linear resin is tailored for blow molded containers that require: Excellent processabilityExcellent ESCRApplications: Typical blow molded applica.. |
|||
Brittleness Temperature | -75.0 °C | -103 °F | ASTM D746 |
DuPont™ Surlyn® 8660 Ionomer Resin, Sodium Surlyn® 8660 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The amount of MAA and neu.. |
|||
Brittleness Temperature | <= -75.0 °C | <= -103 °F | Compression molded parts prepared according to ASTM D 1928, procedure A.; ASTM D746 |
Dow CONTINUUM™ DGDA-2490 NT Bimodal Polyethylene Resin CONTINUUM™ DGDA-2490 NT is produced using UNIPOL™ II process technology. This product may be utilized for pipe applications where long term hydrostatic strength combined with outstanding resistan.. |
|||
Brittleness Temperature | <= -75.0 °C | <= -103 °F | ASTM D746 |
Amco PRIMATOP HDPE 004955HP Blow Molding Polyethylene HDPE 003955PZ features zinc stearate additive and is used for injection blow molding.Former A-Top Polymers product; part of Amco product line since 2013. |
|||
Brittleness Temperature | -75.0 - -70.0 °C | -103 - -94.0 °F | Average value: -70.6 °C Grade Count:8 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Rotational Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Rotational Molding Grade". Each property range of values report.. |
|||
Brittleness Temperature | -75.0 - -70.0 °C | -103 - -94.0 °F | Average value: -70.6 °C Grade Count:9 |
Overview of materials for Linear Medium Density Polyethylene (LMDPE), Film This property data is a summary of similar materials in the MatWeb database for the category "Linear Medium Density Polyethylene (LMDPE), Film". Each property range of values reported is minimum and.. |
|||
Brittleness Temperature | <= -75.0 °C | <= -103 °F | Type A clamp, Type I Specimen; ASTM D746 |
Chevron Phillips Marlex® 9515H High Density Polyethylene, Blow Molding This gas phase, high molecular weight, hexane copolymer with antistatic agent is tailored for lightweight blow molded applications that:Require excellent stiffness to ESCR ratioRequire good melt str.. |
|||
Brittleness Temperature | <= -75.0 °C | <= -103 °F | ASTM D746 |
Ineos H48-500-199 Polyethylene Copolymer This is a high density polyethylene copolymer having a narrow molecular weight distribution. It is intended for roll-out cart applications. This material meets the Food and Drug Administration req.. |
|||
Brittleness Temperature | <= -75.0 °C | <= -103 °F | ASTM D746 |
Ineos HP50-25-153 HDPE A high performance, high density polyethylene copolymer developed for blow molding. It is recommended for use in applications which requiring excellent environmental stress crack resistance (ESCR)... |
|||
Brittleness Temperature | <= -75.0 °C | <= -103 °F | Type A, Type I specimen; ASTM D-746 |
Chevron Phillips Marlex® HHM 5502LW Polyethylene; HDPE High density polyethylene. This high molecular weight, hexene copolymer with synthetic antistatic agent is tailored for lightweight blow molded containers that: Require excellent stiffnessRequire .. |