Material Notes:
Elvax® 40L-08 is an ethylene-vinyl acetate copolymer that is useful in many wire and cable applications because of its excellent mechanical, thermal, and low-smoke properties. The melt index is appropriate for convenient compounding and extrusion. The melt index is consistent because resin molecular weight distribution is controlled to within a relatively narrow range. The molecular weight is high, so finished products will be relatively resistant to mechanical damage and elevated temperatures.Compared with other ethylene-vinyl acetate copolymers, Elvax® 40L-08 contains extremely low amounts of gel, or high molecular weight polymer, that can cause undesirable characteristics in finished productsBecause Elvax® 40L-08 is somewhat crystalline, it is free flowing and does not mass during handling.Typical Applications: Jacketing compounds for automotive ignition and low-smoke cablesStrippable semiconductive shields for power cablesFeatures: Narrow molecular weight distribution and low gel properties for consistent and smooth surfaced finished productsStable, long-term cable performanceInformation provided by DuPont.
Physical Properties Metric English Comments
Density 1.968 g/cc
0.07110 lb/in³
ASTM D1505
Vinyl Acetate Content 40 %
40 %
DuPont Method
Melt Index of Compound 6.0 g/10 min
6.0 g/10 min
ASTM D1238-82
Mechanical Properties Metric English Comments
Hardness, Shore A 53
53
ASTM D2240-82
Tensile Strength at Break 10.8 MPa
1570 psi
ASTM D882-84
Elongation at Break 981 %
981 %
ASTM D882-84
Descriptive Properties Value Comments
Vinyl Acetate Content 40 wt.%
DuPont Method