TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 60 PHR Laminar Filler

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 60 PHR Laminar Filler.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear strength, oil and fuel resistance, and ozone resistance. The life expectancy of urethane is often 5 times longer than other elastomers, thus saving material costs and downtime expense. One shortcoming of polyurethanes is loss of physical properties at temperatures over 180°F (82°C). MILLATHANE HT has overcome this weakness.FormulationMillathane HT100.0Zinc Stearate0.5MBTS4.0MBT2.0THANECURE® ZM1.0Sulfur1.5Laminar60All information provided by TSE Industries
Mechanical Properties Metric English Comments
Hardness, Shore A 62
62
Tensile Strength, Yield 14.01 MPa
2032 psi
Elongation at Yield 479 %
479 %
100% Modulus 0.00267 GPa
0.387 ksi
200% Modulus 0.00395 GPa
0.573 ksi
300% Modulus 0.00530 GPa
0.769 ksi
Tear Strength 30.6 kN/m
175 pli
Die C
Compression Set 52 %

@Temperature 70.0 °C,
Time 79200 sec
52 %

@Temperature 158 °F,
Time 22.0 hour
Processing Properties Metric English Comments
Cure Time 26.0 min

@Temperature 154 °C
0.433 hour

@Temperature 310 °F
Press cured